Atomically Dispersed Nickel Coordinated with Nitrogen on Carbon Nanotubes to Boost Electrochemical CO2 Reduction AITranslate

Korea Institute of Energy Research; Korea Institute of Energy Research; Korea Institute of Energy Research; Korea Institute of Energy Research; Korea Institute of Energy Research; Korea Institute of Energy Research; Korea Advanced Institute of Science and Technology (KAIST); Korea Advanced Institute of Science and Technology (KAIST); Korea Institute of Energy Research
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Single-atom catalysts (SACs) are being widely developed for the CO2 reduction reaction (CO2RR) because of their remarkable activity and selectivity. However, insufficient CO2RR performance and the poor long-term stability of the SACs remain obstacles to process scale-up. Herein, we explore Ni SACs (Ni-N/NCNT) under practical conditions using a zero-gap CO2 electrolyzer for CO production. We demonstrate that the CO2RR performance of the Ni-N/NCNT results from the suitable Ni–N–C, which enhanced electron transfer and increased CO2 adsorption. Furthermore, we propose a strategy for improving the CO2RR performance and long-term stability by focusing on the membrane electrode assembly (MEA) structure. A maximum Faradaic efficiency of 96.73% (at 2.1 V) and partial current density of 219.49 mA cm–2 (at 2.4 V) for CO production were obtained on the MEA with the Ni-N/NCNT catalyst and the Sustainion (Sust.) membrane. In addition, MEA with Sust. exhibited long-term stability at −100 mA cm–2 for over 60 h.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c00933

Chinese Library Classification Number:

Citation Information:

Single-atom catalysts (SACs) are being widely developed for the CO2 reduction reaction (CO2RR) because of their remarkable activity and selectivity. However, insufficient CO2RR performance and the poor long-term stability of the SACs remain obstacles to process scale-up. Herein, we explore Ni SACs (Ni-N/NCNT) under practical conditions using a zero-gap CO2 electrolyzer for CO production. We demonstrate that the CO2RR performance of the Ni-N/NCNT results from the suitable Ni–N–C, which enhanced electron transfer and increased CO2 adsorption. Furthermore, we propose a strategy for improving the CO2RR performance and long-term stability by focusing on the membrane electrode assembly (MEA) structure. A maximum Faradaic efficiency of 96.73% (at 2.1 V) and partial current density of 219.49 mA cm–2 (at 2.4 V) for CO production were obtained on the MEA with the Ni-N/NCNT catalyst and the Sustainion (Sust.) membrane. In addition, MEA with Sust. exhibited long-term stability at −100 mA cm–2 for over 60 h.

quote

GB/T 7714-2015 [1] Young Eun Kim, You Na Ko, ByeongSeon An, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c00933.
MLA [1] Young Eun Kim, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c00933.
APA [1] Young Eun Kim, You Na Ko, ByeongSeon An, Jumi Hong, Ye Eun Jeon, Hak Joo Kim, Seunghyun Lee, Jinwoo Lee, & Wonhee Lee. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c00933
IEEE [1] Young Eun Kim, You Na Ko, ByeongSeon An, Jumi Hong, Ye Eun Jeon, Hak Joo Kim, Seunghyun Lee, Jinwoo Lee, and Wonhee Lee, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c00933.