daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Stable Zinc Metal Anode by Nanosecond Pulsed Laser Enabled Gradient Design AITranslate

Dalian University; Dalian University; Dalian University; Dalian University; Changchun University of Science and Technology; Changchun Institute of Applied Chemistry
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The development of long-term stable Zn anodes capable of operating at high current densities and/or capacities remains a huge challenge. Herein, through the rapid potassium permanganate solution treatment and laser lithography, we have developed a gradient Zn anode (LLP@Treated Zn) with the insulating and hydrophobic passivated-layer at the top and conductive and hydrophilic fresh-zinc-layer at the bottom. This makes the passivation layer prevent the Zn anodes from corrosion and side reactions and induce the preferential deposition of Zn at the bottom of the microchannel without dendrite growth. As a consequence, the LLP@Treated Zn anodes exhibit a stable cycle life for over 700 h at 10 mA cm–2 and 5 mAh cm–2. Moreover, the Zn anodes with different surface morphologies (ring, lattice, etc.) could also be obtained by laser lithography, which proves the flexibility of the pulsed laser lithography strategy in the preparation of battery materials.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c01206

Chinese Library Classification Number:

Citation Information:

The development of long-term stable Zn anodes capable of operating at high current densities and/or capacities remains a huge challenge. Herein, through the rapid potassium permanganate solution treatment and laser lithography, we have developed a gradient Zn anode (LLP@Treated Zn) with the insulating and hydrophobic passivated-layer at the top and conductive and hydrophilic fresh-zinc-layer at the bottom. This makes the passivation layer prevent the Zn anodes from corrosion and side reactions and induce the preferential deposition of Zn at the bottom of the microchannel without dendrite growth. As a consequence, the LLP@Treated Zn anodes exhibit a stable cycle life for over 700 h at 10 mA cm–2 and 5 mAh cm–2. Moreover, the Zn anodes with different surface morphologies (ring, lattice, etc.) could also be obtained by laser lithography, which proves the flexibility of the pulsed laser lithography strategy in the preparation of battery materials.

quote

GB/T 7714-2015 [1] Zhaolin Na, Houkai Qi, Shaohui Li, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c01206.
MLA [1] Zhaolin Na, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c01206.
APA [1] Zhaolin Na, Houkai Qi, Shaohui Li, Yingbin Wu, Qingshuang Wang, & Gang Huang. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c01206
IEEE [1] Zhaolin Na, Houkai Qi, Shaohui Li, Yingbin Wu, Qingshuang Wang, and Gang Huang, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c01206.