Electron Microscopy of Biological Materials at the Nanometer Scale AITranslate

max planck institute of biochemistry; max planck institute of biochemistry; max planck institute of biochemistry
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Electron microscopy of biological matter uses three different imaging modalities: (a) electron crystallography, (b) single-particle analysis, and (c) electron tomography. Ideally, these imaging modalities are applied to frozen-hydrated samples to ensure an optimal preservation of the structures under scrutiny. Cryo-electron microscopy of biological matter has made important advances in the past decades. It has become a research tool that further expands the scope of structural research into unique areas of cell and molecular biology, and it could augment the materials research portfolio in the study of soft and hybrid materials. This review addresses how researchers using transmission electron microscopy can derive structural information at high spatial resolution from fully hydrated specimens, despite their sensitivity to ionizing radiation, despite the adverse conditions of high vacuum for samples that have to be kept in aqueous environments, and despite their low contrast resulting from weakly scattering building blocks.

KeyWords AITranslate

specimen preparation radiation damage frozenhydrated samples cryoelectron tomography singleparticle electron microscopy electron crystallography
No data

Basic Information:

DOI:https://doi.org/10.1146/annurev-matsci-070511-155004

Chinese Library Classification Number:

Citation Information:

Electron microscopy of biological matter uses three different imaging modalities: (a) electron crystallography, (b) single-particle analysis, and (c) electron tomography. Ideally, these imaging modalities are applied to frozen-hydrated samples to ensure an optimal preservation of the structures under scrutiny. Cryo-electron microscopy of biological matter has made important advances in the past decades. It has become a research tool that further expands the scope of structural research into unique areas of cell and molecular biology, and it could augment the materials research portfolio in the study of soft and hybrid materials. This review addresses how researchers using transmission electron microscopy can derive structural information at high spatial resolution from fully hydrated specimens, despite their sensitivity to ionizing radiation, despite the adverse conditions of high vacuum for samples that have to be kept in aqueous environments, and despite their low contrast resulting from weakly scattering building blocks.

quote

GB/T 7714-2015 [1] Lena Fitting Kourkoutis, Jürgen M. Plitzko, Wolfgang Baumeister. Annual Review of Materials Research, 2012(42). DOI:10.1146/annurev-matsci-070511-155004.
MLA [1] Lena Fitting Kourkoutis, et al., Annual Review of Materials Research, no. 42, 2012, https://doi.org/10.1146/annurev-matsci-070511-155004.
APA [1] Lena Fitting Kourkoutis, Jürgen M. Plitzko, & Wolfgang Baumeister. (2012). Annual Review of Materials Research(42). https://doi.org/10.1146/annurev-matsci-070511-155004
IEEE [1] Lena Fitting Kourkoutis, Jürgen M. Plitzko, and Wolfgang Baumeister, Annual Review of Materials Research, no. 42, 2012, doi: 10.1146/annurev-matsci-070511-155004. keywords: {specimen preparation;radiation damage;frozenhydrated samples;cryoelectron tomography;singleparticle electron microscopy;electron crystallography}