Lead halide perovskite nanocrystals (LHP NCs) have emerged as next-generation semiconductor materials with outstanding optical and optoelectronic properties. Because of the high surface-to-volume ratio, the optical and optoelectronic performance and the colloidal stability of LHP NCs largely depend on their surface chemistry, especially the ligands and surface termination. On one hand, the capping ligands improve the colloidal stability and luminescence; on the other hand the highly dynamic binding nature of ligands is detrimental to the colloidal stability and photoluminescence of LHP NCs. In addition, the surface functionalization with desired molecules induces new functionalities such as chirality, light harvesting, and triplet sensitization through energy/electron transfer or use as X-ray detectors. In this review, we present the current understanding of an atomic view of the surface chemistry of colloidal LHP NCs, including crystal termination, vacancies, and different types of capping ligands. Furthermore, we discuss the ligand-induced functionalities, including photocatalysis and chirality.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.2c02363
Chinese Library Classification Number:
Citation Information:
Lead halide perovskite nanocrystals (LHP NCs) have emerged as next-generation semiconductor materials with outstanding optical and optoelectronic properties. Because of the high surface-to-volume ratio, the optical and optoelectronic performance and the colloidal stability of LHP NCs largely depend on their surface chemistry, especially the ligands and surface termination. On one hand, the capping ligands improve the colloidal stability and luminescence; on the other hand the highly dynamic binding nature of ligands is detrimental to the colloidal stability and photoluminescence of LHP NCs. In addition, the surface functionalization with desired molecules induces new functionalities such as chirality, light harvesting, and triplet sensitization through energy/electron transfer or use as X-ray detectors. In this review, we present the current understanding of an atomic view of the surface chemistry of colloidal LHP NCs, including crystal termination, vacancies, and different types of capping ligands. Furthermore, we discuss the ligand-induced functionalities, including photocatalysis and chirality.
quote
| GB/T 7714-2015 | [1] Nadesh FiuzaManeiro, Kun Sun, Iago LópezFernández, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.2c02363. |
| MLA | [1] Nadesh FiuzaManeiro, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.2c02363. |
| APA | [1] Nadesh FiuzaManeiro, Kun Sun, Iago LópezFernández, Sergio GómezGraña, Peter MüllerBuschbaum, & Lakshminarayana Polavarapu. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.2c02363 |
| IEEE | [1] Nadesh FiuzaManeiro, Kun Sun, Iago LópezFernández, Sergio GómezGraña, Peter MüllerBuschbaum, and Lakshminarayana Polavarapu, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.2c02363. |