Quantitative Chemistry in Electrolyte Solvation Design for Aqueous Batteries AITranslate

Lanzhou University; China|University of Science and Technology of China; Lanzhou University;Huzhou Kunlun Enchem Battery Materials Co., Ltd.;Huzhou Kunlun Enchem Battery Materials Co., Ltd.;University of Science and Technology of China; Changchun Institute of Applied Chemistry; Changchun Institute of Applied Chemistry; China|University of Science and Technology of China
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Aqueous electrolyte design is pivotal for boosting the energy density and lifespan of aqueous batteries, because it can expand the electrochemical stability window and also mitigate the parasitic side reactions. Until now, three main kinds of electrolytes, i.e., water-in-salt, eutectic, and additives-modified electrolytes, have been developed by which the activity of H2O can be lowered and/or the formed specific solid–electrolyte interphase (SEI) can mitigate the decomposition of H2O. However, there is still a lack of a universal model to elucidate the reason for the improved performance, especially as the SEI interpretation becomes ever more controversial. Herein, we present a quantitative and graphical model of the electrolyte solvation structure and metal-ion (de)solvation process (i.e., interfacial model) to summarize a relationship between the electrolyte–electrode interfacial chemistry and electrode performance. This Focus Review extends the solvation structure and interfacial model into the field of aqueous electrolytes, revealing the essential influence of the solvation structure’s properties on electrolyte stability and electrode performance, by which electrode performance and electrolyte design can be more quantitatively and accurately understood.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.2c02585

Chinese Library Classification Number:

Citation Information:

Aqueous electrolyte design is pivotal for boosting the energy density and lifespan of aqueous batteries, because it can expand the electrochemical stability window and also mitigate the parasitic side reactions. Until now, three main kinds of electrolytes, i.e., water-in-salt, eutectic, and additives-modified electrolytes, have been developed by which the activity of H2O can be lowered and/or the formed specific solid–electrolyte interphase (SEI) can mitigate the decomposition of H2O. However, there is still a lack of a universal model to elucidate the reason for the improved performance, especially as the SEI interpretation becomes ever more controversial. Herein, we present a quantitative and graphical model of the electrolyte solvation structure and metal-ion (de)solvation process (i.e., interfacial model) to summarize a relationship between the electrolyte–electrode interfacial chemistry and electrode performance. This Focus Review extends the solvation structure and interfacial model into the field of aqueous electrolytes, revealing the essential influence of the solvation structure’s properties on electrolyte stability and electrode performance, by which electrode performance and electrolyte design can be more quantitatively and accurately understood.

quote

GB/T 7714-2015 [1] Leilei Li, Haoran Cheng, Junli Zhang, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.2c02585.
MLA [1] Leilei Li, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.2c02585.
APA [1] Leilei Li, Haoran Cheng, Junli Zhang, Yingjun Guo, Chunsheng Sun, Min Zhou, Qian Li, Zheng Ma, & Jun Ming. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.2c02585
IEEE [1] Leilei Li, Haoran Cheng, Junli Zhang, Yingjun Guo, Chunsheng Sun, Min Zhou, Qian Li, Zheng Ma, and Jun Ming, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.2c02585.