Navigating the Site-Distinct Energy Conversion Properties of Perovskite Quantum Wells AITranslate

University of Macau; University of Macau; National University of Singapore; National University of Singapore; University of Macau; Shenzhen University; University of Macau
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Two-dimensional (2D) halide perovskites (HPs) are self-assembled multi-quantum wells with excitonic peculiarities. They afford favorable moisture and photothermal stability compared to traditional 3D counterparts. However, the energy conversion properties of 2D HPs are highly site-distinct, and they are found to have complicated origins that are associated with diverse local exciton relaxation dynamics, hence causing researchers severe bewilderment when targeting customized applications. This Review intends to offer a thorough survey on this topic. We first introduce the crystallographic structures of 2D HPs and how they render a quantum-well electronic structure. Subsequently, we elaborate on the exciton transport mechanisms in 2D HPs to interpret how excitons arrive at various local sites. Then we concretely introduce the diversiform local/bulk exciton relaxation dynamics that give rise to the wealthy energy conversion attributes. Finally, challenges and opportunities for better understanding and manipulating the exciton dynamics of this promising class of materials are discussed.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.2c02080

Chinese Library Classification Number:

Citation Information:

Two-dimensional (2D) halide perovskites (HPs) are self-assembled multi-quantum wells with excitonic peculiarities. They afford favorable moisture and photothermal stability compared to traditional 3D counterparts. However, the energy conversion properties of 2D HPs are highly site-distinct, and they are found to have complicated origins that are associated with diverse local exciton relaxation dynamics, hence causing researchers severe bewilderment when targeting customized applications. This Review intends to offer a thorough survey on this topic. We first introduce the crystallographic structures of 2D HPs and how they render a quantum-well electronic structure. Subsequently, we elaborate on the exciton transport mechanisms in 2D HPs to interpret how excitons arrive at various local sites. Then we concretely introduce the diversiform local/bulk exciton relaxation dynamics that give rise to the wealthy energy conversion attributes. Finally, challenges and opportunities for better understanding and manipulating the exciton dynamics of this promising class of materials are discussed.

quote

GB/T 7714-2015 [1] Fei Cao, Dejian Yu, Mykola Telychko, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.2c02080.
MLA [1] Fei Cao, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.2c02080.
APA [1] Fei Cao, Dejian Yu, Mykola Telychko, Jiong Lu, Peiyuan Pang, Chenliang Su, & Guichuan Xing. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.2c02080
IEEE [1] Fei Cao, Dejian Yu, Mykola Telychko, Jiong Lu, Peiyuan Pang, Chenliang Su, and Guichuan Xing, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.2c02080.