Toward ultra-long cycling stability and high lithium storage performances: Silica anodes with catalytic effects of low-cost metals particles AITranslate

Yanshan University; Nanjing Tech University;Key Laboratory of Preparation and Applications of Environmental Friendly Materials (Jilin Normal University);Key Laboratory of Preparation and Applications of Environmental Friendly Materials (Jilin Normal University); Changchun Institute of Applied Chemistry; Changchun Institute of Applied Chemistry; Changchun Institute of Applied Chemistry;Key Laboratory of Preparation and Applications of Environmental Friendly Materials (Jilin Normal University)
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

SiO2 has attracted considerable attention for the application of next-generation lithium-ion batteries (LIBs) because of its evident merits, such as large capacity, high natural abundance and low price. Nevertheless, the huge volume inflation and inferior electronic conductivity lead to material degradation and hamper its extensive use. To resolve these challenges, a series of SiO2-M-C (M = Fe, Ni, Cu, C = acetylene black) composites are prepared via a straightforward high energy mechanical milling (HEMM) method. Herein, the M nanoparticles can boost the electronic conductivity and ameliorate electrochemical activity of SiO2 through the catalytic effect of M in breaking Si-O and Li-O bonds, while C can offer a highly conducting assistance to effectively deter agglomeration and pulverization of SiO2 nanoparticles. Superiorly, SiO2-Fe-C reveals exceptional performances with a high initial Coulombic efficiency (CE) of 70.4% at 0.2 A g−1 and long cycle stability under different high current densities (335.6 mAh g−1 at 2 A g−1, 2000 cycles; 212 mAh g−1 at 5 A g−1, 5000 cycles, respectively), which surpasses the reported SiO2-based materials. Considering the convenient preparation and outstanding properties, SiO2-Fe-C can be of visible significance for practical application in next-generation LIBs. Graphic abstract SiO2−M-C (M = Fe, Ni, Cu) composites have been prepared via a simple one-step high energy mechanical milling process. Herein, the M nanoparticles not only can boost the electronic conductivity, but also can ameliorate electrochemical activity of SiO2 through the catalytic effect of M in breaking Si-O and Li-O bonds. SiO2-Fe-C reveals the best electrochemical performances in terms of initial Coulombic efficiency and discharge capacity. Download : Download high-res image (156KB) Download : Download full-size image

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.apmt.2021.101205

Chinese Library Classification Number:

Citation Information:

SiO2 has attracted considerable attention for the application of next-generation lithium-ion batteries (LIBs) because of its evident merits, such as large capacity, high natural abundance and low price. Nevertheless, the huge volume inflation and inferior electronic conductivity lead to material degradation and hamper its extensive use. To resolve these challenges, a series of SiO2-M-C (M = Fe, Ni, Cu, C = acetylene black) composites are prepared via a straightforward high energy mechanical milling (HEMM) method. Herein, the M nanoparticles can boost the electronic conductivity and ameliorate electrochemical activity of SiO2 through the catalytic effect of M in breaking Si-O and Li-O bonds, while C can offer a highly conducting assistance to effectively deter agglomeration and pulverization of SiO2 nanoparticles. Superiorly, SiO2-Fe-C reveals exceptional performances with a high initial Coulombic efficiency (CE) of 70.4% at 0.2 A g−1 and long cycle stability under different high current densities (335.6 mAh g−1 at 2 A g−1, 2000 cycles; 212 mAh g−1 at 5 A g−1, 5000 cycles, respectively), which surpasses the reported SiO2-based materials. Considering the convenient preparation and outstanding properties, SiO2-Fe-C can be of visible significance for practical application in next-generation LIBs. Graphic abstract SiO2−M-C (M = Fe, Ni, Cu) composites have been prepared via a simple one-step high energy mechanical milling process. Herein, the M nanoparticles not only can boost the electronic conductivity, but also can ameliorate electrochemical activity of SiO2 through the catalytic effect of M in breaking Si-O and Li-O bonds. SiO2-Fe-C reveals the best electrochemical performances in terms of initial Coulombic efficiency and discharge capacity. Download : Download high-res image (156KB) Download : Download full-size image

quote

GB/T 7714-2015 [1] Yong Cheng, Bingbing Chen, Mengyao Zhu, et al. Applied Materials Today, 2021(25). DOI:10.1016/j.apmt.2021.101205.
MLA [1] Yong Cheng, et al., Applied Materials Today, no. 25, 2021, https://doi.org/10.1016/j.apmt.2021.101205.
APA [1] Yong Cheng, Bingbing Chen, Mengyao Zhu, Limin Chang, Dongyu Zhang, Chunli Wang, Shaohua Wang, & Limin Wang. (2021). Applied Materials Today(25). https://doi.org/10.1016/j.apmt.2021.101205
IEEE [1] Yong Cheng, Bingbing Chen, Mengyao Zhu, Limin Chang, Dongyu Zhang, Chunli Wang, Shaohua Wang, and Limin Wang, Applied Materials Today, no. 25, 2021, doi: 10.1016/j.apmt.2021.101205.