daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Carbon nanosheet-carbon nanocage encapsulated Cu composite from chemical vapor deposition of real-world plastic waste for tailored CO2 conversion to various products AITranslate

Nanyang Technological University; Nanyang Technological University; Nanyang Technological University; Nanyang Technological University; Nanyang Technological University
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Carbon nanosheet supported Cu (Cu/CNS) is an exemplary electrocatalyst for electrochemical CO2 reduction reaction (CO2RR). The Cu/CNS electrocatalysts however suffer from agglomeration of dispersed Cu nanoparticles and restacking of CNS causing degradation of electrocatalytic activity. Here, a facile one-step method is proposed for manufacturing tailor-made Cu/CNS (e.g., where Cu particle size is stabilized by encapsulation into carbon nanocages (CNC) fixed to a porous and conductive CNS). The electrocatalysts were prepared via catalytic chemical vapor deposition over Cu loaded CaO (Cu/CaO) catalysts from recycled real-world plastic waste. The formation of CNC could help prevent restacking of CNS with specific surface area of around 200–400 m2 g − 1 and maintain good dispersion of Cu nanoparticles. The CO2RR performance (including selectivity and current density) of Cu/CNS was conveniently controlled by the Cu/CaO preparation methods. Compared to Cu/CaO prepared via impregnation or with ethylene glycol, Cu/CaO synthesized via urea-assisted method catalyzed formation of Cu/CNS with improved CO selectivity at lower overpotential (maximum CO Faradaic efficiency was 82.1% at -0.76 V versus reversible hydrogen electrode), higher current density, and suppressed hydrocarbon selectivity owning to the electrocatalyst highest porosity and smallest Cu nanoparticles over CNS. Graphical abstract Download : Download high-res image (136KB) Download : Download full-size image

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.apmt.2021.101207

Chinese Library Classification Number:

Citation Information:

Carbon nanosheet supported Cu (Cu/CNS) is an exemplary electrocatalyst for electrochemical CO2 reduction reaction (CO2RR). The Cu/CNS electrocatalysts however suffer from agglomeration of dispersed Cu nanoparticles and restacking of CNS causing degradation of electrocatalytic activity. Here, a facile one-step method is proposed for manufacturing tailor-made Cu/CNS (e.g., where Cu particle size is stabilized by encapsulation into carbon nanocages (CNC) fixed to a porous and conductive CNS). The electrocatalysts were prepared via catalytic chemical vapor deposition over Cu loaded CaO (Cu/CaO) catalysts from recycled real-world plastic waste. The formation of CNC could help prevent restacking of CNS with specific surface area of around 200–400 m2 g − 1 and maintain good dispersion of Cu nanoparticles. The CO2RR performance (including selectivity and current density) of Cu/CNS was conveniently controlled by the Cu/CaO preparation methods. Compared to Cu/CaO prepared via impregnation or with ethylene glycol, Cu/CaO synthesized via urea-assisted method catalyzed formation of Cu/CNS with improved CO selectivity at lower overpotential (maximum CO Faradaic efficiency was 82.1% at -0.76 V versus reversible hydrogen electrode), higher current density, and suppressed hydrocarbon selectivity owning to the electrocatalyst highest porosity and smallest Cu nanoparticles over CNS. Graphical abstract Download : Download high-res image (136KB) Download : Download full-size image

quote

GB/T 7714-2015 [1] WenQian Chen, Xiaoxu Fu, WeiPing Chan, et al. Applied Materials Today, 2021(25). DOI:10.1016/j.apmt.2021.101207.
MLA [1] WenQian Chen, et al., Applied Materials Today, no. 25, 2021, https://doi.org/10.1016/j.apmt.2021.101207.
APA [1] WenQian Chen, Xiaoxu Fu, WeiPing Chan, Andrei Veksha, & Grzegorz Lisak. (2021). Applied Materials Today(25). https://doi.org/10.1016/j.apmt.2021.101207
IEEE [1] WenQian Chen, Xiaoxu Fu, WeiPing Chan, Andrei Veksha, and Grzegorz Lisak, Applied Materials Today, no. 25, 2021, doi: 10.1016/j.apmt.2021.101207.