Two-dimensional BCN matrix inlaid with single-atom-Cu driven electrochemical nitrate reduction reaction to achieve sustainable industrial-grade production of ammonia AITranslate
Abstract AITranslate
Electrochemical methods have been proven to effectively eliminate nitrates in sewage and convert them into high value-added ammonia products. Here, after annealing treatment of metal boron cluster organic polymers formed by the combination of 1,10-phenanthroline, Cu2+ and closo-[B12H12]2-, a Cu single-atom doped BCN (B-doped CN) with a diamond-shaped nanosheet structure was obtained. In the electrochemical reduction reaction of nitrate, BCN-Cu exhibits excellent catalytic activity, specifically: 1) the ammonia yield rate reached as high as 498.85 μg h−1 cm−2, 1047.14 μg h−1 cm−2, 1900.07 μg h−1 cm−2 and 3358.74 μg h−1 cm−2 at -0.3 V, -0.4 V, -0.5 V and -0.6 V vs reversible hydrogen electrode, respectively, and Faradaic efficiency is 95.90%, 97.28%, 98.23% and 97.37%; 2) after repeated use of BCN-Cu 10 times or continuous operation for 16 h, the activity against electrochemical reduction reaction of nitrate anions is almost unchanged. The 15NO3− isotopic labeling experiment proved that the detected NH3 comes from the reduction of NO3− on BCN-Cu. Control experiments show that the presence of Cu determines whether BCN-Cu has the possibility of catalyzing electrochemical reduction reactions of nitrate, and the presence of the B element enhances the catalytic activity of BCN-Cu. Density functional calculations indicate that in the water phase the process of reducing NO3− to NH3 on Cu0 is an exothermic reaction, and that the adsorption process of NO3− on Cu0 is the rate-determining step. Graphical abstract Single-atom Cu promotes the electrochemical reduction of nitrate in water to high value-added ammonia. Download : Download high-res image (238KB) Download : Download full-size image
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1016/j.apmt.2021.101206
Chinese Library Classification Number:
Citation Information:
Electrochemical methods have been proven to effectively eliminate nitrates in sewage and convert them into high value-added ammonia products. Here, after annealing treatment of metal boron cluster organic polymers formed by the combination of 1,10-phenanthroline, Cu2+ and closo-[B12H12]2-, a Cu single-atom doped BCN (B-doped CN) with a diamond-shaped nanosheet structure was obtained. In the electrochemical reduction reaction of nitrate, BCN-Cu exhibits excellent catalytic activity, specifically: 1) the ammonia yield rate reached as high as 498.85 μg h−1 cm−2, 1047.14 μg h−1 cm−2, 1900.07 μg h−1 cm−2 and 3358.74 μg h−1 cm−2 at -0.3 V, -0.4 V, -0.5 V and -0.6 V vs reversible hydrogen electrode, respectively, and Faradaic efficiency is 95.90%, 97.28%, 98.23% and 97.37%; 2) after repeated use of BCN-Cu 10 times or continuous operation for 16 h, the activity against electrochemical reduction reaction of nitrate anions is almost unchanged. The 15NO3− isotopic labeling experiment proved that the detected NH3 comes from the reduction of NO3− on BCN-Cu. Control experiments show that the presence of Cu determines whether BCN-Cu has the possibility of catalyzing electrochemical reduction reactions of nitrate, and the presence of the B element enhances the catalytic activity of BCN-Cu. Density functional calculations indicate that in the water phase the process of reducing NO3− to NH3 on Cu0 is an exothermic reaction, and that the adsorption process of NO3− on Cu0 is the rate-determining step. Graphical abstract Single-atom Cu promotes the electrochemical reduction of nitrate in water to high value-added ammonia. Download : Download high-res image (238KB) Download : Download full-size image
quote
| GB/T 7714-2015 | [1] Xue Zhao, Xiuxiu Jia, Yingnan He, et al. Applied Materials Today, 2021(25). DOI:10.1016/j.apmt.2021.101206. |
| MLA | [1] Xue Zhao, et al., Applied Materials Today, no. 25, 2021, https://doi.org/10.1016/j.apmt.2021.101206. |
| APA | [1] Xue Zhao, Xiuxiu Jia, Yingnan He, Haibo Zhang, Xiaohai Zhou, Hucai Zhang, Shusheng Zhang, Yemin Dong, Xun Hu, Artem V. Kuklin, Glib V. Baryshnikov, Hans Ågren, & Guangzhi Hu. (2021). Applied Materials Today(25). https://doi.org/10.1016/j.apmt.2021.101206 |
| IEEE | [1] Xue Zhao, Xiuxiu Jia, Yingnan He, Haibo Zhang, Xiaohai Zhou, Hucai Zhang, Shusheng Zhang, Yemin Dong, Xun Hu, Artem V. Kuklin, Glib V. Baryshnikov, Hans Ågren, and Guangzhi Hu, Applied Materials Today, no. 25, 2021, doi: 10.1016/j.apmt.2021.101206. |