Facet-Dependent Control of PbI2 Colloids for over 20% Efficient Perovskite Solar Cells AITranslate
Abstract AITranslate
Organic–inorganic hybrid perovskite-based solar cells (PSCs) have made impressive progress during the past few years, and record power conversion efficiency over 23% has been achieved. However, for solution-processed perovskite films, one of the major challenges for film quality improvement is the lack of a regulation strategy for the colloids in the precursor solution. Here, we demonstrate facet-dependent colloid engineering to adjust the quality of a perovskite film and its photovoltaic performance. This is realized by the development of a facet passivation strategy to synthesize PbI2 (S-PbI2) with tunable morphology. Further, facet-dependent PbI2 colloid regulation is demonstrated, and the relations among the morphology of the PbI2 crystal, features of PbI2 colloids, the morphology of the PbI2 film, and the photovoltaic performance of MAPbI3 are established. The PSCs based on 10% S-PbI2 exhibited a best PCE of 20.22% with improved device reproducibility and hysteresis index compared to that using commercial PbI2 (∼18%).
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.8b02262
Chinese Library Classification Number:
Citation Information:
Organic–inorganic hybrid perovskite-based solar cells (PSCs) have made impressive progress during the past few years, and record power conversion efficiency over 23% has been achieved. However, for solution-processed perovskite films, one of the major challenges for film quality improvement is the lack of a regulation strategy for the colloids in the precursor solution. Here, we demonstrate facet-dependent colloid engineering to adjust the quality of a perovskite film and its photovoltaic performance. This is realized by the development of a facet passivation strategy to synthesize PbI2 (S-PbI2) with tunable morphology. Further, facet-dependent PbI2 colloid regulation is demonstrated, and the relations among the morphology of the PbI2 crystal, features of PbI2 colloids, the morphology of the PbI2 film, and the photovoltaic performance of MAPbI3 are established. The PSCs based on 10% S-PbI2 exhibited a best PCE of 20.22% with improved device reproducibility and hysteresis index compared to that using commercial PbI2 (∼18%).
quote
| GB/T 7714-2015 | [1] Chenxin Ran, Weiyin Gao, Nengxu Li, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.8b02262. |
| MLA | [1] Chenxin Ran, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.8b02262. |
| APA | [1] Chenxin Ran, Weiyin Gao, Nengxu Li, Yingdong Xia, Qi Li, Zhaoxin Wu, Huanping Zhou, Yonghua Chen, Minqiang Wang, & Wei Huang. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.8b02262 |
| IEEE | [1] Chenxin Ran, Weiyin Gao, Nengxu Li, Yingdong Xia, Qi Li, Zhaoxin Wu, Huanping Zhou, Yonghua Chen, Minqiang Wang, and Wei Huang, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.8b02262. |