daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Iridium-Triggered Phase Transition of MoS2 Nanosheets Boosts Overall Water Splitting in Alkaline Media AITranslate

Jilin University; Jilin University; Jilin University; Jilin University; Institute of Physics; Institute of Physics; Jilin University; Institute of High Energy Physics; Jilin University; Jilin University; Jilin University; Jilin University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Metallic phase molybdenum disulfide (1T-MoS2), with its fast carrier mobility and highly abundant active sites, plays a vital role in the field of catalysis. However, the development of a simple and efficient strategy for the preparation of stabilized 1T-MoS2 remains a great challenge. Herein, we report the spontaneous phase transformation of MoS2 from the 2H to the 1T phase, caused by the strong metal–support interaction during iridium (Ir) adsorption. The resulting Ir/MoS2 heterostructures show higher catalytic activity for overall water splitting than those of commercial Pt/C and IrO2 in alkaline media. We believe that the spontaneous phase transformation of this material not only opens up a new perspective for developing advanced catalysts for alkaline water splitting but also presents an efficient and intriguing method for the phase engineering of two-dimensional materials.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.8b01840

Chinese Library Classification Number:

Citation Information:

Metallic phase molybdenum disulfide (1T-MoS2), with its fast carrier mobility and highly abundant active sites, plays a vital role in the field of catalysis. However, the development of a simple and efficient strategy for the preparation of stabilized 1T-MoS2 remains a great challenge. Herein, we report the spontaneous phase transformation of MoS2 from the 2H to the 1T phase, caused by the strong metal–support interaction during iridium (Ir) adsorption. The resulting Ir/MoS2 heterostructures show higher catalytic activity for overall water splitting than those of commercial Pt/C and IrO2 in alkaline media. We believe that the spontaneous phase transformation of this material not only opens up a new perspective for developing advanced catalysts for alkaline water splitting but also presents an efficient and intriguing method for the phase engineering of two-dimensional materials.

quote

GB/T 7714-2015 [1] Shuting Wei, Xiaoqiang Cui, Yanchao Xu, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.8b01840.
MLA [1] Shuting Wei, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.8b01840.
APA [1] Shuting Wei, Xiaoqiang Cui, Yanchao Xu, Bo Shang, Qinghua Zhang, Lin Gu, Xiaofeng Fan, Lirong Zheng, Changmin Hou, Haihua Huang, Sisi Wen, & Weitao Zheng. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.8b01840
IEEE [1] Shuting Wei, Xiaoqiang Cui, Yanchao Xu, Bo Shang, Qinghua Zhang, Lin Gu, Xiaofeng Fan, Lirong Zheng, Changmin Hou, Haihua Huang, Sisi Wen, and Weitao Zheng, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.8b01840.