Abstract AITranslate

The two-electron water oxidation reaction (2e-WOR) is a promising route for distributed electrochemical synthesis of hydrogen peroxide (H2O2), an effective and green oxidizer, bleaching agent, and antiseptic. To date, the best electrocatalyst for 2e-WOR, in terms of selectivity against the competing 4e-WOR to form O2, is BiVO4. Nevertheless, BiVO4 is unstable and has a high overpotential of ∼340 mV at 0.2 mA/cm2 for 2e-WOR. Herein, we use density functional theory to identify a new, efficient, selective, and stable electrocatalyst for 2e-WOR, i.e., the ternary oxide calcium stannate (CaSnO3). Our experiments show that CaSnO3 achieves an overpotential of 230 mV at 0.2 mA/cm2, peak Faraday efficiency of 76% for 2e-WOR at 3.2 V vs the reversible hydrogen electrode (RHE), and stable performance for over 12 h, outperforming BiVO4 in all aspects. This work demonstrates the promise of CaSnO3 as a selective and cost-effective electrocatalyst candidate for H2O2 production from water oxidation.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.8b02303

Chinese Library Classification Number:

Citation Information:

The two-electron water oxidation reaction (2e-WOR) is a promising route for distributed electrochemical synthesis of hydrogen peroxide (H2O2), an effective and green oxidizer, bleaching agent, and antiseptic. To date, the best electrocatalyst for 2e-WOR, in terms of selectivity against the competing 4e-WOR to form O2, is BiVO4. Nevertheless, BiVO4 is unstable and has a high overpotential of ∼340 mV at 0.2 mA/cm2 for 2e-WOR. Herein, we use density functional theory to identify a new, efficient, selective, and stable electrocatalyst for 2e-WOR, i.e., the ternary oxide calcium stannate (CaSnO3). Our experiments show that CaSnO3 achieves an overpotential of 230 mV at 0.2 mA/cm2, peak Faraday efficiency of 76% for 2e-WOR at 3.2 V vs the reversible hydrogen electrode (RHE), and stable performance for over 12 h, outperforming BiVO4 in all aspects. This work demonstrates the promise of CaSnO3 as a selective and cost-effective electrocatalyst candidate for H2O2 production from water oxidation.

quote

GB/T 7714-2015 [1] So Yeon Park, Hadi Abroshan, Xinjian Shi, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.8b02303.
MLA [1] So Yeon Park, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.8b02303.
APA [1] So Yeon Park, Hadi Abroshan, Xinjian Shi, Hyun Suk Jung, Samira Siahrostami, & Xiaolin Zheng. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.8b02303
IEEE [1] So Yeon Park, Hadi Abroshan, Xinjian Shi, Hyun Suk Jung, Samira Siahrostami, and Xiaolin Zheng, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.8b02303.