Nanotomography Investigation of 3D Printed Batteries with a Water-in-Salt Gel Polymer Electrolyte AITranslate

Stony Brook University; Brookhaven National Laboratory; Stony Brook University; Stony Brook University; Brookhaven National Laboratory; Brookhaven National Laboratory; Brookhaven National Laboratory; Stony Brook University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

3D printing, also known as additive manufacturing, has emerged as a promising strategy to design and fabricate future energy storage devices. Although significant progress has been reported, current 3D printed battery designs are still limited by the choice of the electrolyte, such as ceramic or conventional toxic organic electrolytes. Here, we incorporated the latest developments in aqueous batteries into a novel 3D printable battery that can be fabricated directly in an ambient environment that is also more environmentally friendly. Specifically, a gel polymer electrolyte with a water-in-salt concept was introduced in our 3D-printed batteries. Combining their advantages, the resulting 3D printable batteries show promise for much simplified processing conditions. The structural, (electro-)chemical, and morphological evolution batteries are being investigated by synchrotron X-ray nanotomography and electrochemical analysis. Overall, our research explores the possibility of an easier and more environmentally friendly way to build 3D printable, customizable batteries for future technologies.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.2c01133

Chinese Library Classification Number:

Citation Information:

3D printing, also known as additive manufacturing, has emerged as a promising strategy to design and fabricate future energy storage devices. Although significant progress has been reported, current 3D printed battery designs are still limited by the choice of the electrolyte, such as ceramic or conventional toxic organic electrolytes. Here, we incorporated the latest developments in aqueous batteries into a novel 3D printable battery that can be fabricated directly in an ambient environment that is also more environmentally friendly. Specifically, a gel polymer electrolyte with a water-in-salt concept was introduced in our 3D-printed batteries. Combining their advantages, the resulting 3D printable batteries show promise for much simplified processing conditions. The structural, (electro-)chemical, and morphological evolution batteries are being investigated by synchrotron X-ray nanotomography and electrochemical analysis. Overall, our research explores the possibility of an easier and more environmentally friendly way to build 3D printable, customizable batteries for future technologies.

quote

GB/T 7714-2015 [1] Dean Yen, ChengHung Lin, David J. Sprouster, et al. ACS Materials Letters, 2023(5). DOI:10.1021/acsmaterialslett.2c01133.
MLA [1] Dean Yen, et al., ACS Materials Letters, no. 5, 2023, https://doi.org/10.1021/acsmaterialslett.2c01133.
APA [1] Dean Yen, ChengHung Lin, David J. Sprouster, Xiaoying Zheng, Xianghui Xiao, WahKeat Lee, Mingyuan Ge, & Yuchen Karen ChenWiegart. (2023). ACS Materials Letters(5). https://doi.org/10.1021/acsmaterialslett.2c01133
IEEE [1] Dean Yen, ChengHung Lin, David J. Sprouster, Xiaoying Zheng, Xianghui Xiao, WahKeat Lee, Mingyuan Ge, and Yuchen Karen ChenWiegart, ACS Materials Letters, no. 5, 2023, doi: 10.1021/acsmaterialslett.2c01133.