Low-Temperature Plasma-Enhanced Atomic Layer Deposition of ZnMgO for Efficient CZTS Solar Cells AITranslate

School of Photovoltaic and Renewable Energy Engineering, UNSW Sydney;School of Photovoltaic and Renewable Energy Engineering, UNSW Sydney;School of Photovoltaic and Renewable Energy Engineering, UNSW Sydney;School of Photovoltaic and Renewable Energy Engineering, UNSW Sydney;School of Photovoltaic and Renewable Energy Engineering, UNSW Sydney;School of Photovoltaic and Renewable Energy Engineering, UNSW Sydney;School of Photovoltaic and Renewable Energy Engineering, UNSW Sydney;School of Photovoltaic and Renewable Energy Engineering, UNSW Sydney;School of Photovoltaic and Renewable Energy Engineering, UNSW Sydney
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Cu2ZnSnS4 (CZTS) solar cells are an emerging photovoltaic technology owing to their earth abundance, all-dry processability, and environmental friendliness. Further power conversion efficiency enhancement of the Cd-free CZTS device necessitates the substitution of traditionally used intrinsic ZnO by an alternative wide-band-gap window layer. Here, we demonstrate deposition of a ZnMgO window layer of controlled thickness, composition, and electro-optical properties by atomic layer deposition (ALD). The amorphous ZnMgO deposited at low temperature down to 100 °C using plasma-enhanced ALD showed smoothness superior to that of high-temperature plasma-enhanced ALD and doping density comparable to that of high-temperature thermal ALD but with a much lower electron affinity. The overall charge carrier recombination at the CZTS/ZnSnO/ZnMgO region was reduced due to the optimized ZnMgO conduction band minimum, thus reducing the VOC value and fill factor loss for a CZTS solar cell. In addition, the thinner- and larger-band-gap ZnMgO was believed to reduce the parasitic absorption, improving the JSC value and boosting the efficiency to 10%.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.2c01203

Chinese Library Classification Number:

Citation Information:

Cu2ZnSnS4 (CZTS) solar cells are an emerging photovoltaic technology owing to their earth abundance, all-dry processability, and environmental friendliness. Further power conversion efficiency enhancement of the Cd-free CZTS device necessitates the substitution of traditionally used intrinsic ZnO by an alternative wide-band-gap window layer. Here, we demonstrate deposition of a ZnMgO window layer of controlled thickness, composition, and electro-optical properties by atomic layer deposition (ALD). The amorphous ZnMgO deposited at low temperature down to 100 °C using plasma-enhanced ALD showed smoothness superior to that of high-temperature plasma-enhanced ALD and doping density comparable to that of high-temperature thermal ALD but with a much lower electron affinity. The overall charge carrier recombination at the CZTS/ZnSnO/ZnMgO region was reduced due to the optimized ZnMgO conduction band minimum, thus reducing the VOC value and fill factor loss for a CZTS solar cell. In addition, the thinner- and larger-band-gap ZnMgO was believed to reduce the parasitic absorption, improving the JSC value and boosting the efficiency to 10%.

quote

GB/T 7714-2015 [1] Xin Cui, Kaiwen Sun, Jialiang Huang, et al. ACS Materials Letters, 2023(5). DOI:10.1021/acsmaterialslett.2c01203.
MLA [1] Xin Cui, et al., ACS Materials Letters, no. 5, 2023, https://doi.org/10.1021/acsmaterialslett.2c01203.
APA [1] Xin Cui, Kaiwen Sun, Jialiang Huang, Heng Sun, Ao Wang, Xiaojie Yuan, Martin Green, Bram Hoex, & Xiaojing Hao. (2023). ACS Materials Letters(5). https://doi.org/10.1021/acsmaterialslett.2c01203
IEEE [1] Xin Cui, Kaiwen Sun, Jialiang Huang, Heng Sun, Ao Wang, Xiaojie Yuan, Martin Green, Bram Hoex, and Xiaojing Hao, ACS Materials Letters, no. 5, 2023, doi: 10.1021/acsmaterialslett.2c01203.