Fabrication and Condensate Microdrop Self-Propelling of Biomimetic Nanostructured Polymer Surfaces without Chemical Modification AITranslate

South China University of Technology; South China University of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Condensate microdrop self-propelling (CMDSP) can occur on the cicada wing surfaces due to very low solid–liquid adhesion of the closely packed nanopillars. A promising and industrial strategy is proposed for successively replicating the nanopillars on the cicada wing onto the polypropylene (PP) surfaces. Its process includes nickel replica fabrication and PP replica injection molding. Packed nanopillars with nanoscale interspaces endow the PP replicas with CMDSP functionality. Mechanism for the CMDSP on the PP replica is analyzed. This work should be the first report of achieving the CMDSP function on polymer surfaces without chemical modification, which is favorable for industrial applications such as anti-icing/frosting and enhanced condensation heat transfer.

KeyWords AITranslate

biomimetic surface condensate microdrop selfpropelling cicada wing nanostructure polymer injection molding
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.9b00200

Chinese Library Classification Number:

Citation Information:

Condensate microdrop self-propelling (CMDSP) can occur on the cicada wing surfaces due to very low solid–liquid adhesion of the closely packed nanopillars. A promising and industrial strategy is proposed for successively replicating the nanopillars on the cicada wing onto the polypropylene (PP) surfaces. Its process includes nickel replica fabrication and PP replica injection molding. Packed nanopillars with nanoscale interspaces endow the PP replicas with CMDSP functionality. Mechanism for the CMDSP on the PP replica is analyzed. This work should be the first report of achieving the CMDSP function on polymer surfaces without chemical modification, which is favorable for industrial applications such as anti-icing/frosting and enhanced condensation heat transfer.

quote

GB/T 7714-2015 [1] HanXiong Huang, Yue An. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00200.
MLA [1] HanXiong Huang, and Yue An. ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00200.
APA [1] HanXiong Huang, & Yue An. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00200
IEEE [1] HanXiong Huang and Yue An, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.9b00200. keywords: {biomimetic surface;condensate microdrop selfpropelling;cicada wing;nanostructure;polymer injection molding}