Low-k and Recyclable High-Performance POSS/Polyamide Composites Based on Diels–Alder Reaction AITranslate

Donghua University; Donghua University; Donghua University; Donghua University; Donghua University; Donghua University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The rapid development in electronics requires high-performance and low-k materials. Introducing additional recyclability to these materials could further promote their application from environmental and economic aspects. In this paper, we report a reversibly cross-linked composite from a newly designed maleimide functionalized POSS (mPOSS) and aromatic polyamide with pendent furan groups (POF). The Diels–Alder reaction between maleimide and furan groups allowed the facile cross-linking of POF by mPOSS, thus significantly improving the thermal and mechanical properties of mPOSS/POF composites. The reversible feature of Diels–Alder reaction also conferred good recyclability to the mPOSS/POF composites. Tensile tests suggested that more than 80% of mechanical properties were retained in reprocessed composites even with multiple reprocessing cycles. Moreover, the porous nature of POSS molecules and the restricted motion of polymer chains by cross-linking significantly reduced the dielectric constant and dielectric loss of composites. These fascinating features of our mPOSS/POF composites make them promising candidate for high-performance, recyclable, and low-k dielectrics.

KeyWords AITranslate

polyaimde POSS Diels−Alder reaction recycling dielectric constant
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.8b00215

Chinese Library Classification Number:

Citation Information:

The rapid development in electronics requires high-performance and low-k materials. Introducing additional recyclability to these materials could further promote their application from environmental and economic aspects. In this paper, we report a reversibly cross-linked composite from a newly designed maleimide functionalized POSS (mPOSS) and aromatic polyamide with pendent furan groups (POF). The Diels–Alder reaction between maleimide and furan groups allowed the facile cross-linking of POF by mPOSS, thus significantly improving the thermal and mechanical properties of mPOSS/POF composites. The reversible feature of Diels–Alder reaction also conferred good recyclability to the mPOSS/POF composites. Tensile tests suggested that more than 80% of mechanical properties were retained in reprocessed composites even with multiple reprocessing cycles. Moreover, the porous nature of POSS molecules and the restricted motion of polymer chains by cross-linking significantly reduced the dielectric constant and dielectric loss of composites. These fascinating features of our mPOSS/POF composites make them promising candidate for high-performance, recyclable, and low-k dielectrics.

quote

GB/T 7714-2015 [1] Kaiju Luo, Guocheng Song, Yan Wang, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.8b00215.
MLA [1] Kaiju Luo, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.8b00215.
APA [1] Kaiju Luo, Guocheng Song, Yan Wang, Junrong Yu, Jing Zhu, & Zuming Hu. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.8b00215
IEEE [1] Kaiju Luo, Guocheng Song, Yan Wang, Junrong Yu, Jing Zhu, and Zuming Hu, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.8b00215. keywords: {polyaimde;POSS;Diels−Alder reaction;recycling;dielectric constant}