Impact of Cathode Material Particle Size on the Capacity of Bulk-Type All-Solid-State Batteries AITranslate
Abstract AITranslate
The implementation of all-solid-state batteries (ASSBs) is regarded as an important step toward next-generation energy storage systems, in particular for electric vehicles and portable electronics. This may be achieved through application of layered Ni-rich oxide cathode materials such as Li1+x(Ni1–y–zCoyMnz)1–xO2 (NCM) with high specific capacity and thiophosphate-based solid electrolytes. Here, the profound effect that the secondary particle size of the cathode active material has on the capacity of ASSB cells comprising NCM622 (60% Ni), β-Li3PS4, and In anode is demonstrated. We show the benefits of using small particles (d ≪ 10 μm), allowing virtually full charge capacity. This finding is rationalized through galvanostatic charge–discharge tests and complementary ex situ and operando X-ray diffraction experiments combined with Rietveld refinement analysis. Our results indicate the importance of considering and avoiding electrochemically inactive electrode material in bulk-type ASSBs, which we show using charge transport measurements is due to poor electronic contact (in carbon-free cathode composites).
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.8b00275
Chinese Library Classification Number:
Citation Information:
The implementation of all-solid-state batteries (ASSBs) is regarded as an important step toward next-generation energy storage systems, in particular for electric vehicles and portable electronics. This may be achieved through application of layered Ni-rich oxide cathode materials such as Li1+x(Ni1–y–zCoyMnz)1–xO2 (NCM) with high specific capacity and thiophosphate-based solid electrolytes. Here, the profound effect that the secondary particle size of the cathode active material has on the capacity of ASSB cells comprising NCM622 (60% Ni), β-Li3PS4, and In anode is demonstrated. We show the benefits of using small particles (d ≪ 10 μm), allowing virtually full charge capacity. This finding is rationalized through galvanostatic charge–discharge tests and complementary ex situ and operando X-ray diffraction experiments combined with Rietveld refinement analysis. Our results indicate the importance of considering and avoiding electrochemically inactive electrode material in bulk-type ASSBs, which we show using charge transport measurements is due to poor electronic contact (in carbon-free cathode composites).
quote
| GB/T 7714-2015 | [1] Florian Strauss, Timo Bartsch, Lea de Biasi, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b00275. |
| MLA | [1] Florian Strauss, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b00275. |
| APA | [1] Florian Strauss, Timo Bartsch, Lea de Biasi, AYoung Kim, Jürgen Janek, Pascal Hartmann, & Torsten Brezesinski. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b00275 |
| IEEE | [1] Florian Strauss, Timo Bartsch, Lea de Biasi, AYoung Kim, Jürgen Janek, Pascal Hartmann, and Torsten Brezesinski, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b00275. |