Identifying the Active Site of N-Doped Graphene for Oxygen Reduction by Selective Chemical Modification AITranslate
Abstract AITranslate
N-doped carbon materials are promising electrocatalysts for oxygen reduction reaction (ORR). However, the lack of knowledge in the nature of active sites limits the rational design of this type of catalysts. Although pyridinic N species are proposed to be active for ORR, little experimental evidence is provided to reveal the reactive sites. Herein, we developed a surface-modification method to identify the ortho-carbon atom of the pyridinic ring as the reactive site for ORR on N-doped graphene. The pyridinic ring of N-doped graphene was selectively grafted by an acetyl group at pyridinic N and ortho-C atoms by electrophilic and radical substitution, respectively. The former remained most of ORR catalytic activity, while the latter lost its activity completely. DFT calculations confirm that O2 can get adsorbed and reduced favorably on the ortho-C atom of the pyridinic ring. This study provides new insight into the nature of active sites and the ORR mechanism for N-doped carbon materials.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.8b00258
Chinese Library Classification Number:
Citation Information:
N-doped carbon materials are promising electrocatalysts for oxygen reduction reaction (ORR). However, the lack of knowledge in the nature of active sites limits the rational design of this type of catalysts. Although pyridinic N species are proposed to be active for ORR, little experimental evidence is provided to reveal the reactive sites. Herein, we developed a surface-modification method to identify the ortho-carbon atom of the pyridinic ring as the reactive site for ORR on N-doped graphene. The pyridinic ring of N-doped graphene was selectively grafted by an acetyl group at pyridinic N and ortho-C atoms by electrophilic and radical substitution, respectively. The former remained most of ORR catalytic activity, while the latter lost its activity completely. DFT calculations confirm that O2 can get adsorbed and reduced favorably on the ortho-C atom of the pyridinic ring. This study provides new insight into the nature of active sites and the ORR mechanism for N-doped carbon materials.
quote
| GB/T 7714-2015 | [1] Tao Wang, ZhiXin Chen, YuGang Chen, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b00258. |
| MLA | [1] Tao Wang, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b00258. |
| APA | [1] Tao Wang, ZhiXin Chen, YuGang Chen, LiJun Yang, XiaoDong Yang, JinYu Ye, HaiPing Xia, ZhiYou Zhou, & ShiGang Sun. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b00258 |
| IEEE | [1] Tao Wang, ZhiXin Chen, YuGang Chen, LiJun Yang, XiaoDong Yang, JinYu Ye, HaiPing Xia, ZhiYou Zhou, and ShiGang Sun, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b00258. |