daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Unilamellar Metallic MoS2/Graphene Superlattice for Efficient Sodium Storage and Hydrogen Evolution AITranslate

National Institute for Materials Science (NIMS); National Institute for Materials Science (NIMS); National Institute for Materials Science (NIMS); National Institute for Materials Science (NIMS); National Institute for Materials Science (NIMS)
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Unilamellar metallic nanosheets possess superiority for electrochemical energy storage and conversion applications compared to the few-layered bulk and semiconducting counterparts. Here, we report the utilization of unilamellar metallic 1T phase MoS2 nanosheets for efficient sodium storage and hydrogen evolution through a MoS2/graphene superlattice. The superlattice-like assembly composed of alternately restacked unilamellar MoS2 and modified reduced graphene oxide nanosheets was prepared by a facile solution-phase direct restacking method. As an anode for sodium storage, the MoS2/graphene superlattice anode exhibited an excellent rate capability of ∼240 mA h g–1 at 51.2 A g–1 and a stable reversible capacity of ∼380 mA h g–1 after 1000 cycles at 10 A g–1. In addition, a low onset potential of ∼88 mV and a small Tafel slope of 48.7 mV decade–1 were attained for the hydrogen evolution reaction. Our findings are important for further developing the potential of 2D nanosheets for energy storage and conversion.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.8b00110

Chinese Library Classification Number:

Citation Information:

Unilamellar metallic nanosheets possess superiority for electrochemical energy storage and conversion applications compared to the few-layered bulk and semiconducting counterparts. Here, we report the utilization of unilamellar metallic 1T phase MoS2 nanosheets for efficient sodium storage and hydrogen evolution through a MoS2/graphene superlattice. The superlattice-like assembly composed of alternately restacked unilamellar MoS2 and modified reduced graphene oxide nanosheets was prepared by a facile solution-phase direct restacking method. As an anode for sodium storage, the MoS2/graphene superlattice anode exhibited an excellent rate capability of ∼240 mA h g–1 at 51.2 A g–1 and a stable reversible capacity of ∼380 mA h g–1 after 1000 cycles at 10 A g–1. In addition, a low onset potential of ∼88 mV and a small Tafel slope of 48.7 mV decade–1 were attained for the hydrogen evolution reaction. Our findings are important for further developing the potential of 2D nanosheets for energy storage and conversion.

quote

GB/T 7714-2015 [1] Pan Xiong, Renzhi Ma, Nobuyuki Sakai, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b00110.
MLA [1] Pan Xiong, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b00110.
APA [1] Pan Xiong, Renzhi Ma, Nobuyuki Sakai, Leanddas Nurdiwijayanto, & Takayoshi Sasaki. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b00110
IEEE [1] Pan Xiong, Renzhi Ma, Nobuyuki Sakai, Leanddas Nurdiwijayanto, and Takayoshi Sasaki, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b00110.