Deformation characteristics and inertial effect of complex aluminum alloy sheet part under impact hydroforming: experiments and numerical analysis AITranslate

University of Science and Technology of China; University of Science and Technology of China; University of Science and Technology of China; University of Science and Technology of China;Physical-Technical Institute;Physical-Technical Institute
AITranslate
Publisher: Springer Nature
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Impact hydroforming (IHF), as a novel sheet metal forming technology with the advantages of high strain rate forming and flexible liquid loading, is highly suitable for efficiently manufacturing aluminum complex-shaped sheet parts. In this paper, deformation characteristics of complex sheet parts under IHF are systematically investigated. The mechanical properties of 2024 aluminum alloy under a wide range of strain rates (10−3 s−1–3.3×103 s−1) were studied. It indicated that the elongation of 2024 aluminum alloy was improved by 116.01% under strain rates of 3.306 × 103 s−1, referring to 10−3 s−1. Further, a complex-shaped part with symmetrical and asymmetrical structures was selected. The deformation characteristics of sheet and role of inertial effect under IHF were investigated with well-developed solid–liquid coupling finite element (SLC-FE) model with high accuracy. Differentiating deformation tendency is found for symmetrical structure with notably prior deformation at central zone, showing a “bulging” profile at initial forming stage. Whereas, synchronous deformation is presented for asymmetrical structure with a “flat” profile. Additionally, distinctive inertial effect was observed at different positions change for both symmetrical and asymmetrical structures, in which lower values were resulted at their central regions. Meanwhile, the inertial effect evolved with the impacting speed. Specially, larger difference of inertial effect was observed with increasing impacting speed.

KeyWords AITranslate

2024 aluminum alloy Impact hydroforming High strain rate Inertial effect
No data

Basic Information:

DOI:https://doi.org/10.1007/s40436-022-00430-0

Chinese Library Classification Number:

Citation Information:

Impact hydroforming (IHF), as a novel sheet metal forming technology with the advantages of high strain rate forming and flexible liquid loading, is highly suitable for efficiently manufacturing aluminum complex-shaped sheet parts. In this paper, deformation characteristics of complex sheet parts under IHF are systematically investigated. The mechanical properties of 2024 aluminum alloy under a wide range of strain rates (10−3 s−1–3.3×103 s−1) were studied. It indicated that the elongation of 2024 aluminum alloy was improved by 116.01% under strain rates of 3.306 × 103 s−1, referring to 10−3 s−1. Further, a complex-shaped part with symmetrical and asymmetrical structures was selected. The deformation characteristics of sheet and role of inertial effect under IHF were investigated with well-developed solid–liquid coupling finite element (SLC-FE) model with high accuracy. Differentiating deformation tendency is found for symmetrical structure with notably prior deformation at central zone, showing a “bulging” profile at initial forming stage. Whereas, synchronous deformation is presented for asymmetrical structure with a “flat” profile. Additionally, distinctive inertial effect was observed at different positions change for both symmetrical and asymmetrical structures, in which lower values were resulted at their central regions. Meanwhile, the inertial effect evolved with the impacting speed. Specially, larger difference of inertial effect was observed with increasing impacting speed.

quote

GB/T 7714-2015 [1] LiangLiang Xia, ShiHong Zhang, Yong Xu, et al. Advances in Manufacturing, 2023(11). DOI:10.1007/s40436-022-00430-0.
MLA [1] LiangLiang Xia, et al., Advances in Manufacturing, no. 11, 2023, https://doi.org/10.1007/s40436-022-00430-0.
APA [1] LiangLiang Xia, ShiHong Zhang, Yong Xu, ShuaiFeng Chen, Boris B. Khina, & Artur I. Pokrovsky. (2023). Advances in Manufacturing(11). https://doi.org/10.1007/s40436-022-00430-0
IEEE [1] LiangLiang Xia, ShiHong Zhang, Yong Xu, ShuaiFeng Chen, Boris B. Khina, and Artur I. Pokrovsky, Advances in Manufacturing, no. 11, 2023, doi: 10.1007/s40436-022-00430-0. keywords: {2024 aluminum alloy;Impact hydroforming;High strain rate;Inertial effect}