Size effects on process performance and product quality in progressive microforming of shafted gears revealed by experiment and numerical modeling AITranslate

The Hong Kong Polytechnic University; The Hong Kong Polytechnic University; The Hong Kong Polytechnic University
AITranslate
Publisher: Springer Nature
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

As one of the indispensable actuating components in micro-systems, the shafted microgear is in great production demand. Microforming is a manufacturing process to produce microgears to meet the needs. Due to the small geometrical size, there are uncertain process performance and product quality issues in this production process. In this study, the shafted microgears were fabricated in two different scaling factors with four grain sizes using a progressively extrusion-blanking method. To explore the unknown of the process, grain-based modeling was proposed and employed to simulate the entire forming process. The results show that when the grains are large, the anisotropy of single grains has an obvious size effect on the forming behavior and process performance; and the produced geometries and surface quality are worsened; and the deformation load is decreased. Five deformation zones were identified in the microstructures with different hardness and distributions of stress and strain. The simulation by using the proposed model successfully predicted the formation of zones and revealed the inhomogeneous deformation in the forming process. The undesirable geometries of microgears including material unfilling, burr and inclination were observed on the shaft and teeth of gear, and the inclination size is increased obviously with grain size. To avoid the formation of inclination and material unfilling, the punch was redesigned, and a die insert was added to constraint the bottom surface of the gear teeth. The new products had then the better forming quality.

KeyWords AITranslate

Microforming Microprocess performance Microforming quality Size effect affected deformation behavior Die design optimization
No data

Basic Information:

DOI:https://doi.org/10.1007/s40436-022-00414-0

Chinese Library Classification Number:

Citation Information:

As one of the indispensable actuating components in micro-systems, the shafted microgear is in great production demand. Microforming is a manufacturing process to produce microgears to meet the needs. Due to the small geometrical size, there are uncertain process performance and product quality issues in this production process. In this study, the shafted microgears were fabricated in two different scaling factors with four grain sizes using a progressively extrusion-blanking method. To explore the unknown of the process, grain-based modeling was proposed and employed to simulate the entire forming process. The results show that when the grains are large, the anisotropy of single grains has an obvious size effect on the forming behavior and process performance; and the produced geometries and surface quality are worsened; and the deformation load is decreased. Five deformation zones were identified in the microstructures with different hardness and distributions of stress and strain. The simulation by using the proposed model successfully predicted the formation of zones and revealed the inhomogeneous deformation in the forming process. The undesirable geometries of microgears including material unfilling, burr and inclination were observed on the shaft and teeth of gear, and the inclination size is increased obviously with grain size. To avoid the formation of inclination and material unfilling, the punch was redesigned, and a die insert was added to constraint the bottom surface of the gear teeth. The new products had then the better forming quality.

quote

GB/T 7714-2015 [1] JunYuan Zheng, Hui Liu, MingWang Fu. Advances in Manufacturing, 2023(11). DOI:10.1007/s40436-022-00414-0.
MLA [1] JunYuan Zheng, et al., Advances in Manufacturing, no. 11, 2023, https://doi.org/10.1007/s40436-022-00414-0.
APA [1] JunYuan Zheng, Hui Liu, & MingWang Fu. (2023). Advances in Manufacturing(11). https://doi.org/10.1007/s40436-022-00414-0
IEEE [1] JunYuan Zheng, Hui Liu, and MingWang Fu, Advances in Manufacturing, no. 11, 2023, doi: 10.1007/s40436-022-00414-0. keywords: {Microforming;Microprocess performance;Microforming quality;Size effect affected deformation behavior;Die design optimization}