daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Precision wire electrochemical machining of thick structures in powder superalloy René 88DT using a partially insulated tube electrode AITranslate

Nanjing University of Aeronautics and Astronautics; Nanjing University of Aeronautics and Astronautics; Nanjing University of Aeronautics and Astronautics; Nanjing University of Aeronautics and Astronautics
AITranslate
Publisher: Springer Nature
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Wire electrochemical machining (WECM) is a potential method for manufacturing macrostructures from difficult-to-cut materials, such as turbine slots, with good surface integrity and low costs. In this study, a novel tube electrode with array holes in the front and insulation in the back was applied using WECM to improve the machining precision and efficiency. Additionally, assisted by an immersion electrolyte and axial flushing, the electrolyte-deficient gap was supplemented to achieve the cutting of a very thick workpiece. The simulation results indicated that this method could effectively reduce the machining gap and improve the uniformity of the electric- and flow-field distributions. Experiments verified that when the uninsulated range (machining angle) was reduced from 360° to 90°, the side machining gap was reduced from 462.5 µm to 175 µm. Finally, using optimized machining parameters, array slits with gaps as small as (175±10) μm were machined on a powder superalloy René 88DT sample with a thickness of 10 mm at a feed rate of 16 µm/s. The feasibility of fabricating complex profiles using this method was verified using a self-designed servo device.

KeyWords AITranslate

Wire electrochemical machining (WECM) Tube electrode Partial insulation Machining angle Electrolyte flushing Surface quality
No data

Basic Information:

DOI:https://doi.org/10.1007/s40436-023-00441-5

Chinese Library Classification Number:

Citation Information:

Wire electrochemical machining (WECM) is a potential method for manufacturing macrostructures from difficult-to-cut materials, such as turbine slots, with good surface integrity and low costs. In this study, a novel tube electrode with array holes in the front and insulation in the back was applied using WECM to improve the machining precision and efficiency. Additionally, assisted by an immersion electrolyte and axial flushing, the electrolyte-deficient gap was supplemented to achieve the cutting of a very thick workpiece. The simulation results indicated that this method could effectively reduce the machining gap and improve the uniformity of the electric- and flow-field distributions. Experiments verified that when the uninsulated range (machining angle) was reduced from 360° to 90°, the side machining gap was reduced from 462.5 µm to 175 µm. Finally, using optimized machining parameters, array slits with gaps as small as (175±10) μm were machined on a powder superalloy René 88DT sample with a thickness of 10 mm at a feed rate of 16 µm/s. The feasibility of fabricating complex profiles using this method was verified using a self-designed servo device.

quote

GB/T 7714-2015 [1] Cheng Tang, Zhao Han, ZhongQi Zhou, et al. Advances in Manufacturing, 2023(11). DOI:10.1007/s40436-023-00441-5.
MLA [1] Cheng Tang, et al., Advances in Manufacturing, no. 11, 2023, https://doi.org/10.1007/s40436-023-00441-5.
APA [1] Cheng Tang, Zhao Han, ZhongQi Zhou, & XiaoLong Fang. (2023). Advances in Manufacturing(11). https://doi.org/10.1007/s40436-023-00441-5
IEEE [1] Cheng Tang, Zhao Han, ZhongQi Zhou, and XiaoLong Fang, Advances in Manufacturing, no. 11, 2023, doi: 10.1007/s40436-023-00441-5. keywords: {Wire electrochemical machining (WECM);Tube electrode;Partial insulation;Machining angle;Electrolyte flushing;Surface quality}