Free-Standing Flexible Composite Film That Is Transparent, Omnipohobic, and Resistant against Steel Wool Abrasion AITranslate

Queen’s University; Queen’s University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The encapsulating film of current foldable smartphone touchscreens consists of a flexible, colorless polyimide substrate, layered stepwise with a top hard coat, an antireflection coat, and last with an outermost antifingerprint layer. A flexible polymer substrate is essential to overcoming the inherent bendability limitations of the hard coat. This study explores a different approach to encapsulating film fabrication. This method involves the infusion of GPOSS (octakis(3-glycidyloxypropyl)silsesquioxane), GPOSS-FC6 (GPOSS with a perfluorinated hexyl group), and a cationic ring-opening initiator into electrospun nylon nanofiber mat pores and subsequently photocuring the GPOSS mixture to create a composite. The resulting film is transparent, omniphobic, and remarkably flexible. A 40 μm thick free-standing composite film alone can endure over 1000 bending cycles with a 1 mm radius without cracking. Additionally, it exhibits superior wear resistance by withstanding hundreds of steel wool abrasions, surpassing that of a cured neat F-GPOSS hard coating. This study highlights the remarkable reinforcing effect of electrospun nanofibers on hard materials, enhancing simultaneously the normally exclusive properties: flexibility and abrasion resistance. The reported material should find applications in various fields beyond foldable touchscreens.

KeyWords AITranslate

omniphobicity composite nanofiber electrospinning POSS coatings
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c02190

Chinese Library Classification Number:

Citation Information:

The encapsulating film of current foldable smartphone touchscreens consists of a flexible, colorless polyimide substrate, layered stepwise with a top hard coat, an antireflection coat, and last with an outermost antifingerprint layer. A flexible polymer substrate is essential to overcoming the inherent bendability limitations of the hard coat. This study explores a different approach to encapsulating film fabrication. This method involves the infusion of GPOSS (octakis(3-glycidyloxypropyl)silsesquioxane), GPOSS-FC6 (GPOSS with a perfluorinated hexyl group), and a cationic ring-opening initiator into electrospun nylon nanofiber mat pores and subsequently photocuring the GPOSS mixture to create a composite. The resulting film is transparent, omniphobic, and remarkably flexible. A 40 μm thick free-standing composite film alone can endure over 1000 bending cycles with a 1 mm radius without cracking. Additionally, it exhibits superior wear resistance by withstanding hundreds of steel wool abrasions, surpassing that of a cured neat F-GPOSS hard coating. This study highlights the remarkable reinforcing effect of electrospun nanofibers on hard materials, enhancing simultaneously the normally exclusive properties: flexibility and abrasion resistance. The reported material should find applications in various fields beyond foldable touchscreens.

quote

GB/T 7714-2015 [1] Sean Chun Keat Tan, Guojun Liu. ACS Applied Polymer Materials, 2024(6). DOI:10.1021/acsapm.3c02190.
MLA [1] Sean Chun Keat Tan, and Guojun Liu. ACS Applied Polymer Materials, no. 6, 2024, https://doi.org/10.1021/acsapm.3c02190.
APA [1] Sean Chun Keat Tan, & Guojun Liu. (2024). ACS Applied Polymer Materials(6). https://doi.org/10.1021/acsapm.3c02190
IEEE [1] Sean Chun Keat Tan and Guojun Liu, ACS Applied Polymer Materials, no. 6, 2024, doi: 10.1021/acsapm.3c02190. keywords: {omniphobicity;composite;nanofiber;electrospinning;POSS;coatings}