Abstract AITranslate

Daytime radiative cooling has generated an escalating level of interest as it offers zero-energy cooling even under strong solar illumination. However, two issues remain unresolved regarding the daytime radiative cooling. One is to further improve the cooling effect at high temperatures and the other is to suppress overcooling at low temperatures. Herein, we approached an effective design of a radiative cooling composite enhanced by a phase change material (PCM). The incorporation of the PCM increases the subambient cooling temperature of the composite by 2 °C under a solar intensity of ∼850 W m–2, resulting in a final cooling effect of 6.8 °C, which demonstrates the synergistic enhancement of the radiative cooling in hot conditions. Furthermore, the incorporation of the PCM slows down the cooling rate of the composite when the temperature drops below the crystallization point, indicating a great potential to mitigate overcooling in cold environments. Additionally, the resulting composite exhibits excellent thermal and shape stabilities. Overall, the proposed PCM-enhanced radiative cooling composite demonstrates a significant advance toward the radiative cooling regulation, which holds promise for broadening its application in various practical environments.

KeyWords AITranslate

radiative cooling phase change material overcooling solar reflectance infrared emittance
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c02194

Chinese Library Classification Number:

Citation Information:

Daytime radiative cooling has generated an escalating level of interest as it offers zero-energy cooling even under strong solar illumination. However, two issues remain unresolved regarding the daytime radiative cooling. One is to further improve the cooling effect at high temperatures and the other is to suppress overcooling at low temperatures. Herein, we approached an effective design of a radiative cooling composite enhanced by a phase change material (PCM). The incorporation of the PCM increases the subambient cooling temperature of the composite by 2 °C under a solar intensity of ∼850 W m–2, resulting in a final cooling effect of 6.8 °C, which demonstrates the synergistic enhancement of the radiative cooling in hot conditions. Furthermore, the incorporation of the PCM slows down the cooling rate of the composite when the temperature drops below the crystallization point, indicating a great potential to mitigate overcooling in cold environments. Additionally, the resulting composite exhibits excellent thermal and shape stabilities. Overall, the proposed PCM-enhanced radiative cooling composite demonstrates a significant advance toward the radiative cooling regulation, which holds promise for broadening its application in various practical environments.

quote

GB/T 7714-2015 [1] Bo Xiang, Peng Xu, Renzhi Li, et al. ACS Applied Polymer Materials, 2024(6). DOI:10.1021/acsapm.3c02194.
MLA [1] Bo Xiang, et al., ACS Applied Polymer Materials, no. 6, 2024, https://doi.org/10.1021/acsapm.3c02194.
APA [1] Bo Xiang, Peng Xu, Renzhi Li, & Rong Zhang. (2024). ACS Applied Polymer Materials(6). https://doi.org/10.1021/acsapm.3c02194
IEEE [1] Bo Xiang, Peng Xu, Renzhi Li, and Rong Zhang, ACS Applied Polymer Materials, no. 6, 2024, doi: 10.1021/acsapm.3c02194. keywords: {radiative cooling;phase change material;overcooling;solar reflectance;infrared emittance}