Cyclotriphosphonitrile-Based Electroactive Flame-Retardant Polymers for Electrochromic/Supercapacitor Devices AITranslate
Abstract AITranslate
To mitigate the thermal runaway issue and thereby enhance the safety of electrochemical energy storage devices, designing electro-active materials with intrinsic flame-retardant and thermal insulation functions is considered an effective way. Herein, we propose an innovative molecular design strategy that amalgamated the cyclotriphosphonitrile derivative HCTP-BTDPBr with a conjugated polymer framework to construct intrinsic flame-retardant electro-active materials serving as dual function electrochromic/supercapacitor applications. Two series of donor–acceptor type copolymers, namely, PrOEG-BTDx-CTPy and PrOC12-BTDx-CTPy, were prepared by carefully modulating the ratio of HCTP-BTDPBr in the whole polymers. Systematic characterization of the electrochemical and flame-retardant performance revealed that PrOEG-BTD0.82-CTP0.18, PrOC12-BTD0.46-CTP0.54, and PrOC12-CTP showed obvious flame-retardant effects with the ignition times of 120, 108, and 80 s alongside heat release rates of 41.9, 27.5, and 31 KW m–2 g–1, respectively. The high specific capacitance of 87.34 mF cm–2 (at 0.1 mA cm–2) was obtained from PrOEG-BTD0.82-CTP0.18. Meanwhile, those three copolymers showed excellent electrochromic performance with multiple color changes between blue/transparent, purple/gray, and red-orange/grass green and impressive coloration efficiencies of 258, 158, and 172 cm2 C1–, respectively. Thus, we believe this molecular design strategy has great potential to improve the safety of electrochemical energy storage devices.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.3c02043
Chinese Library Classification Number:
Citation Information:
To mitigate the thermal runaway issue and thereby enhance the safety of electrochemical energy storage devices, designing electro-active materials with intrinsic flame-retardant and thermal insulation functions is considered an effective way. Herein, we propose an innovative molecular design strategy that amalgamated the cyclotriphosphonitrile derivative HCTP-BTDPBr with a conjugated polymer framework to construct intrinsic flame-retardant electro-active materials serving as dual function electrochromic/supercapacitor applications. Two series of donor–acceptor type copolymers, namely, PrOEG-BTDx-CTPy and PrOC12-BTDx-CTPy, were prepared by carefully modulating the ratio of HCTP-BTDPBr in the whole polymers. Systematic characterization of the electrochemical and flame-retardant performance revealed that PrOEG-BTD0.82-CTP0.18, PrOC12-BTD0.46-CTP0.54, and PrOC12-CTP showed obvious flame-retardant effects with the ignition times of 120, 108, and 80 s alongside heat release rates of 41.9, 27.5, and 31 KW m–2 g–1, respectively. The high specific capacitance of 87.34 mF cm–2 (at 0.1 mA cm–2) was obtained from PrOEG-BTD0.82-CTP0.18. Meanwhile, those three copolymers showed excellent electrochromic performance with multiple color changes between blue/transparent, purple/gray, and red-orange/grass green and impressive coloration efficiencies of 258, 158, and 172 cm2 C1–, respectively. Thus, we believe this molecular design strategy has great potential to improve the safety of electrochemical energy storage devices.
quote
| GB/T 7714-2015 | [1] Hong Xu, Jiaoyi Ning, Zunbin Duan, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c02043. |
| MLA | [1] Hong Xu, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c02043. |
| APA | [1] Hong Xu, Jiaoyi Ning, Zunbin Duan, Bin Deng, Dinghui Chen, Manyu Liu, Hongyang Li, Yulu Cai, Yaowu He, & Hong Meng. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c02043 |
| IEEE | [1] Hong Xu, Jiaoyi Ning, Zunbin Duan, Bin Deng, Dinghui Chen, Manyu Liu, Hongyang Li, Yulu Cai, Yaowu He, and Hong Meng, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c02043. keywords: {thermal runaway;flameretardant polymer;cyclotriphosphonitrile;electrochromism;supercapacitor} |