Electrochemically Initiated Synthesis of Polyacrylamide Microgels and Core-shell Particles AITranslate

Institute of Physical Chemistry;Institute of Physical Chemistry;Institute of Physical Chemistry; Cardinal Stefan Wyszynski University in Warsaw;Institute of Physical Chemistry
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Herein, we developed a simple procedure for synthesizing micrometer-sized microgel particles as a suspension in an aqueous solution and thin films deposited as shells on different inorganic cores. A sufficiently high constant potential was applied to the working electrode to commence the initiator decomposition that resulted in gelation. Under hydrodynamic conditions, this initiation allowed preparing different morphology microgels at room temperature. Importantly, neither heating nor UV-light illumination was needed to initiate the polymerization. Moreover, thin films of the cross-linked gel were anchored on different core substrates, including silica and magnetic nanoparticles. Scanning electron microscopy and transmission electron microscopy imaging confirmed the microgel particles’ and films’ irregular shape and porous structure. Energy-dispersive X-ray spectroscopy indicated that the core coating with the microgel film was successful. Dynamic light scattering measured the micrometer size of gel particles with different combinations of acrylic monomers. Thermogravimetric analysis and the first-derivative thermogravimetric analysis revealed that the microgels’ thermal stability of different compositions was different. Fourier-transform infrared and 13C NMR spectroscopy showed successful copolymerization of the main, functional, and cross-linking monomers.

KeyWords AITranslate

electrochemical polymerization initiation hydrodynamic electropolymerization microgel coreshell particle inorganic core
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c01359

Chinese Library Classification Number:

Citation Information:

Herein, we developed a simple procedure for synthesizing micrometer-sized microgel particles as a suspension in an aqueous solution and thin films deposited as shells on different inorganic cores. A sufficiently high constant potential was applied to the working electrode to commence the initiator decomposition that resulted in gelation. Under hydrodynamic conditions, this initiation allowed preparing different morphology microgels at room temperature. Importantly, neither heating nor UV-light illumination was needed to initiate the polymerization. Moreover, thin films of the cross-linked gel were anchored on different core substrates, including silica and magnetic nanoparticles. Scanning electron microscopy and transmission electron microscopy imaging confirmed the microgel particles’ and films’ irregular shape and porous structure. Energy-dispersive X-ray spectroscopy indicated that the core coating with the microgel film was successful. Dynamic light scattering measured the micrometer size of gel particles with different combinations of acrylic monomers. Thermogravimetric analysis and the first-derivative thermogravimetric analysis revealed that the microgels’ thermal stability of different compositions was different. Fourier-transform infrared and 13C NMR spectroscopy showed successful copolymerization of the main, functional, and cross-linking monomers.

quote

GB/T 7714-2015 [1] Nabila Yasmeen, Jakub Kalecki, Pawel Borowicz, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.1c01359.
MLA [1] Nabila Yasmeen, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.1c01359.
APA [1] Nabila Yasmeen, Jakub Kalecki, Pawel Borowicz, Wlodzimierz Kutner, & Piyush S. Sharma. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.1c01359
IEEE [1] Nabila Yasmeen, Jakub Kalecki, Pawel Borowicz, Wlodzimierz Kutner, and Piyush S. Sharma, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.1c01359. keywords: {electrochemical polymerization initiation;hydrodynamic electropolymerization;microgel;coreshell particle;inorganic core}