daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Mechanochromic Responses of Cholesteric Liquid Crystal Droplets with Nanoscale Periodic Helical Structures Showing Reversible and Tunable Structural Color AITranslate

Zhejiang University; Zhejiang University; Zhejiang University; Zhejiang University; Zhejiang University; The Hong Kong University of Science and Technology; Korea Advanced Institute of Science and Technology; Zhejiang University; Tsinghua University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Cholesteric liquid crystal (CLC) droplets with nanoscale periodic helical structures are omnidirectional under planar anchoring, and light is selectively reflected from the droplet center at all directions. However, when CLC droplets are too small, random light scattering dominates. In this regard, we present a facile method to increase the selective Bragg reflection of CLC droplets and demonstrate the unique mechanochromic responses of CLC-droplet-dispersed polymer films. The films are originally opaque and white, when the films are bidirectionally stretched, spherical CLC droplets are squeezed into oblate shape and the point defect at the center of each CLC droplet transitions to a ring defect, greatly increasing the selective Bragg reflection region and resulting in the appearance of structural color. By tuning the helical pitches via the chiral dopant concentration from 1.7 to 3.0 wt %, the desired structural color is achieved. Smart sensors show color changes in response to hydration and dehydration are designed, paving the way for the developments of CLC-based functional materials and smart devices.

KeyWords AITranslate

nanostructure liquid crystal cholesteric structural color stimulus response
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c01362

Chinese Library Classification Number:

Citation Information:

Cholesteric liquid crystal (CLC) droplets with nanoscale periodic helical structures are omnidirectional under planar anchoring, and light is selectively reflected from the droplet center at all directions. However, when CLC droplets are too small, random light scattering dominates. In this regard, we present a facile method to increase the selective Bragg reflection of CLC droplets and demonstrate the unique mechanochromic responses of CLC-droplet-dispersed polymer films. The films are originally opaque and white, when the films are bidirectionally stretched, spherical CLC droplets are squeezed into oblate shape and the point defect at the center of each CLC droplet transitions to a ring defect, greatly increasing the selective Bragg reflection region and resulting in the appearance of structural color. By tuning the helical pitches via the chiral dopant concentration from 1.7 to 3.0 wt %, the desired structural color is achieved. Smart sensors show color changes in response to hydration and dehydration are designed, paving the way for the developments of CLC-based functional materials and smart devices.

quote

GB/T 7714-2015 [1] Chenjing Yang, Baiheng Wu, Jian Ruan, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.1c01362.
MLA [1] Chenjing Yang, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.1c01362.
APA [1] Chenjing Yang, Baiheng Wu, Jian Ruan, Peng Zhao, Jianzhen Shan, Rui Zhang, Dong Ki Yoon, Dong Chen, & Kai Liu. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.1c01362
IEEE [1] Chenjing Yang, Baiheng Wu, Jian Ruan, Peng Zhao, Jianzhen Shan, Rui Zhang, Dong Ki Yoon, Dong Chen, and Kai Liu, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.1c01362. keywords: {nanostructure;liquid crystal;cholesteric;structural color;stimulus response}