Double-Shelled Ni–Fe–P/N-Doped Carbon Nanobox Derived from a Prussian Blue Analogue as an Electrode Material for K-Ion Batteries and Li–S Batteries AITranslate
Abstract AITranslate
Rational design, convenient fabrication, and application of double-shelled hollow architectures with well-defined morphology and multicompositions as electrodes for rechargeable batteries still remain great challenges. Herein, double-shelled Ni–Fe–P/N-doped carbon nanoboxes (defined as Ni–Fe–P/NC) were synthesized and then applied as electrode materials for potassium-ion batteries (KIBs) and Li–S batteries, first. The unique architectures could not only alleviate volume changes and prevent aggregation of Ni–Fe–P/NC during cycling but could also provide efficient surface areas for infiltration of electrolyte. Additionally, nitrogen-doped carbon could improve the conductivity of the electrode. Hence, when these Ni–Fe–P/NC nanoboxes were applied as anode materials for KIBs, they delivered enhanced cycling stability (172.9 mA h g–1 after 1600 cycles at 500 mA g–1 and 115 mA h g–1 after 2600 cycles at 1000 mA g–1). Meanwhile, the Ni–Fe–P/NC could also be used as the sulfur host material for Li–S batteries; benefiting from its unique hollow structure, it can accommodate high sulfur loading and have strong chemical adsorption ability to polysulfides.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.9b00573
Chinese Library Classification Number:
Citation Information:
Rational design, convenient fabrication, and application of double-shelled hollow architectures with well-defined morphology and multicompositions as electrodes for rechargeable batteries still remain great challenges. Herein, double-shelled Ni–Fe–P/N-doped carbon nanoboxes (defined as Ni–Fe–P/NC) were synthesized and then applied as electrode materials for potassium-ion batteries (KIBs) and Li–S batteries, first. The unique architectures could not only alleviate volume changes and prevent aggregation of Ni–Fe–P/NC during cycling but could also provide efficient surface areas for infiltration of electrolyte. Additionally, nitrogen-doped carbon could improve the conductivity of the electrode. Hence, when these Ni–Fe–P/NC nanoboxes were applied as anode materials for KIBs, they delivered enhanced cycling stability (172.9 mA h g–1 after 1600 cycles at 500 mA g–1 and 115 mA h g–1 after 2600 cycles at 1000 mA g–1). Meanwhile, the Ni–Fe–P/NC could also be used as the sulfur host material for Li–S batteries; benefiting from its unique hollow structure, it can accommodate high sulfur loading and have strong chemical adsorption ability to polysulfides.
quote
| GB/T 7714-2015 | [1] Xiaoxia Chen, Suyuan Zeng, Haliya Muheiyati, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b00573. |
| MLA | [1] Xiaoxia Chen, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b00573. |
| APA | [1] Xiaoxia Chen, Suyuan Zeng, Haliya Muheiyati, YanJun Zhai, Chuanchuan Li, Xuyang Ding, Lu Wang, Debao Wang, Liqiang Xu, Yanyan He, & Yitai Qian. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b00573 |
| IEEE | [1] Xiaoxia Chen, Suyuan Zeng, Haliya Muheiyati, YanJun Zhai, Chuanchuan Li, Xuyang Ding, Lu Wang, Debao Wang, Liqiang Xu, Yanyan He, and Yitai Qian, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.9b00573. |