Institute of Technology Sligo; King Abdullah University of Science and Technology (KAUST); King Abdullah University of Science and Technology (KAUST); King Abdullah University of Science and Technology (KAUST); Institute of Technology Sligo; Institute of Technology Sligo; University of Cincinnati; Institute of Technology Sligo
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The photocatalytic water splitting technique is a promising alternative to produce hydrogen using a facile and proficient method. In the current Review, recent progress made in photocatalytic hydrogen evolution reaction (HER) using 2D nanomaterials (NMs) and composite heterostructures is described. The strong in-plane chemical bonds along with weak van der Waals interaction make these materials lucrative for surface-related applications. State-of-the-art protocols designed for the synthesis of 2D NMs is discussed in detail. The Review illustrates density functional theory (DFT)-based studies against the new set of 2D NMs, which also highlights the importance of structural defects and doping in the electronic structure. Additionally, the Review describes the influence of electronic, structural, and surface manipulation strategies. These impact the electronic structures, intrinsic conductivity, and finally output toward HER. Moreover, this Review also provides a fresh perspective on the prospects and challenges existing behind the application and fabrication strategies.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.9b00940

Chinese Library Classification Number:

Citation Information:

The photocatalytic water splitting technique is a promising alternative to produce hydrogen using a facile and proficient method. In the current Review, recent progress made in photocatalytic hydrogen evolution reaction (HER) using 2D nanomaterials (NMs) and composite heterostructures is described. The strong in-plane chemical bonds along with weak van der Waals interaction make these materials lucrative for surface-related applications. State-of-the-art protocols designed for the synthesis of 2D NMs is discussed in detail. The Review illustrates density functional theory (DFT)-based studies against the new set of 2D NMs, which also highlights the importance of structural defects and doping in the electronic structure. Additionally, the Review describes the influence of electronic, structural, and surface manipulation strategies. These impact the electronic structures, intrinsic conductivity, and finally output toward HER. Moreover, this Review also provides a fresh perspective on the prospects and challenges existing behind the application and fabrication strategies.

quote

GB/T 7714-2015 [1] Priyanka Ganguly, Moussab Harb, Zhen Cao, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b00940.
MLA [1] Priyanka Ganguly, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b00940.
APA [1] Priyanka Ganguly, Moussab Harb, Zhen Cao, Luigi Cavallo, Ailish Breen, Saoirse Dervin, Dionysios D. Dionysiou, & Suresh C. Pillai. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b00940
IEEE [1] Priyanka Ganguly, Moussab Harb, Zhen Cao, Luigi Cavallo, Ailish Breen, Saoirse Dervin, Dionysios D. Dionysiou, and Suresh C. Pillai, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.9b00940.