daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Light-Driven Chemical Looping for Ammonia Synthesis AITranslate

Rice University; Rice University; Rice University; Rice University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Synthetic ammonia has been the primary worldwide source of agricultural fertilizer over the last century and is a promising carbon-free energy carrier for sustainable transportation. Despite its global importance, synthetic ammonia produced with the Haber–Bosch process is extremely energy- and resource-intensive. Here we demonstrate a three-step chemical looping strategy to produce ammonia using only light, natural gas, nitrogen, and water. Titanium nitride nanoparticles were utilized as plasmonic antennas to assist the transformation of magnesium-based nanomaterials through oxide, metallic, and nitride phases under optical illumination. All reactions were performed and monitored in situ using frequency-modulated rotational spectroscopy, which allowed the experiments to take advantage of the rotational spectra’s unique sensitivity to isotopic labeling to monitor and verify key reaction intermediates. This validation of a light-driven process for the synthesis of ammonia demonstrates an innovative route toward photosynthetic production of essential chemical commodities.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.9b00860

Chinese Library Classification Number:

Citation Information:

Synthetic ammonia has been the primary worldwide source of agricultural fertilizer over the last century and is a promising carbon-free energy carrier for sustainable transportation. Despite its global importance, synthetic ammonia produced with the Haber–Bosch process is extremely energy- and resource-intensive. Here we demonstrate a three-step chemical looping strategy to produce ammonia using only light, natural gas, nitrogen, and water. Titanium nitride nanoparticles were utilized as plasmonic antennas to assist the transformation of magnesium-based nanomaterials through oxide, metallic, and nitride phases under optical illumination. All reactions were performed and monitored in situ using frequency-modulated rotational spectroscopy, which allowed the experiments to take advantage of the rotational spectra’s unique sensitivity to isotopic labeling to monitor and verify key reaction intermediates. This validation of a light-driven process for the synthesis of ammonia demonstrates an innovative route toward photosynthetic production of essential chemical commodities.

quote

GB/T 7714-2015 [1] Dayne F. Swearer, Nicola R. Knowles, Henry O. Everitt, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b00860.
MLA [1] Dayne F. Swearer, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b00860.
APA [1] Dayne F. Swearer, Nicola R. Knowles, Henry O. Everitt, & Naomi J. Halas. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b00860
IEEE [1] Dayne F. Swearer, Nicola R. Knowles, Henry O. Everitt, and Naomi J. Halas, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.9b00860.