MAPbCl3-Mediated Decomposition Process to Tune Cl/PbI2 Distribution in MAPbI3 Films AITranslate

PR China|Qingdao University of Science and Technology; PR China|Qingdao University of Science and Technology;Qingdao University of Science and Technology;Qingdao Institute of Bioenergy and Bioprocess Technology;Qingdao Institute of Bioenergy and Bioprocess Technology;Qingdao Institute of Bioenergy and Bioprocess Technology;Qingdao Institute of Bioenergy and Bioprocess Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Various methods have been developed to optimize the active layer of perovskite solar cells. To date, the introduction of excess PbI2 and chlorine doping are two typical means. Herein, an ion exchange–decomposition process was designed to combine these two approaches. In this process, the I–Cl exchange and MACl sublimation occurred simultaneously at elevated temperature, resulting in a PbI2-excess, Cl-doped perovskite film. This combined strategy could guarantee that as much chlorine as possible was doped into the perovskite crystal lattice, which enables the production of perovskite films with obviously reduced defect density and enhanced carrier diffusion length. Strikingly, the power conversion efficiency of the device is boosted from 17.17% to 20.15%.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.8b00837

Chinese Library Classification Number:

Citation Information:

Various methods have been developed to optimize the active layer of perovskite solar cells. To date, the introduction of excess PbI2 and chlorine doping are two typical means. Herein, an ion exchange–decomposition process was designed to combine these two approaches. In this process, the I–Cl exchange and MACl sublimation occurred simultaneously at elevated temperature, resulting in a PbI2-excess, Cl-doped perovskite film. This combined strategy could guarantee that as much chlorine as possible was doped into the perovskite crystal lattice, which enables the production of perovskite films with obviously reduced defect density and enhanced carrier diffusion length. Strikingly, the power conversion efficiency of the device is boosted from 17.17% to 20.15%.

quote

GB/T 7714-2015 [1] Cuiping Zhang, Zhipeng Li, Juan Liu, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b00837.
MLA [1] Cuiping Zhang, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b00837.
APA [1] Cuiping Zhang, Zhipeng Li, Juan Liu, Yunchuan Xin, Zhipeng Shao, Guanglei Cui, & Shuping Pang. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b00837
IEEE [1] Cuiping Zhang, Zhipeng Li, Juan Liu, Yunchuan Xin, Zhipeng Shao, Guanglei Cui, and Shuping Pang, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b00837.