Planar FAPbBr3 Solar Cells with Power Conversion Efficiency above 10% AITranslate
Abstract AITranslate
Bromide-based hybrid perovskites are of particular interest not only due to the fact that they offer a way to go beyond the Shockley–Queisser limit via the tandem cell scheme but single-junction devices of them can also achieve reasonably high efficiency with high stability for solar energy conversion. However, the highest power conversion efficiency achieved up to now for FAPbBr3 single-junction solar cells is only 8.2%, which is far below the efficiency of ∼17% predicted from detailed balance analysis. Here, a two-step method (the intermolecule exchange pathway) was systematically optimized for the fabrication of high-quality FAPbBr3 films. A molecule of urea, structurally similar to formamidinium, is introduced as an additive to tune the intermolecular ion exchange procedure. SnO2 is introduced as an electron-selective contact to the planar structured FAPbBr3 solar cells. As a result, a power conversion efficiency of 10.61% and a Voc of 1.56 V are achieved with planar structured solar cells, both of which represent the highest value ever reported for FAPbBr3 solar cells.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.8b00540
Chinese Library Classification Number:
Citation Information:
Bromide-based hybrid perovskites are of particular interest not only due to the fact that they offer a way to go beyond the Shockley–Queisser limit via the tandem cell scheme but single-junction devices of them can also achieve reasonably high efficiency with high stability for solar energy conversion. However, the highest power conversion efficiency achieved up to now for FAPbBr3 single-junction solar cells is only 8.2%, which is far below the efficiency of ∼17% predicted from detailed balance analysis. Here, a two-step method (the intermolecule exchange pathway) was systematically optimized for the fabrication of high-quality FAPbBr3 films. A molecule of urea, structurally similar to formamidinium, is introduced as an additive to tune the intermolecular ion exchange procedure. SnO2 is introduced as an electron-selective contact to the planar structured FAPbBr3 solar cells. As a result, a power conversion efficiency of 10.61% and a Voc of 1.56 V are achieved with planar structured solar cells, both of which represent the highest value ever reported for FAPbBr3 solar cells.
quote
| GB/T 7714-2015 | [1] Yongfei Zhang, Yongqi Liang, Yajuan Wang, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b00540. |
| MLA | [1] Yongfei Zhang, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b00540. |
| APA | [1] Yongfei Zhang, Yongqi Liang, Yajuan Wang, Fengwan Guo, Licheng Sun, & Dongsheng Xu. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b00540 |
| IEEE | [1] Yongfei Zhang, Yongqi Liang, Yajuan Wang, Fengwan Guo, Licheng Sun, and Dongsheng Xu, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b00540. |