Monolithic Photoelectrochemical Device for Direct Water Splitting with 19% Efficiency AITranslate
Abstract AITranslate
Efficient unassisted solar water splitting, a pathway to storable renewable energy in the form of chemical bonds, requires optimization of a photoelectrochemical device based on photovoltaic tandem heterojunctions. We report a monolithic photocathode device architecture that exhibits significantly reduced surface reflectivity, minimizing parasitic light absorption and reflection losses. A tailored multifunctional crystalline titania interphase layer acts as a corrosion protection layer, with favorable band alignment between the semiconductor conduction band and the energy level for water reduction, facilitating electron transport at the cathode–electrolyte interface. It also provides a favorable substrate for adhesion of high-activity Rh catalyst nanoparticles. Under simulated AM 1.5G irradiation, solar-to-hydrogen efficiencies of 19.3 and 18.5% are obtained in acidic and neutral electrolytes, respectively. The system reaches a value of 0.85 of the theoretical limit for photoelectrochemical water splitting for the energy gap combination employed in the tandem-junction photoelectrode structure.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.8b00920
Chinese Library Classification Number:
Citation Information:
Efficient unassisted solar water splitting, a pathway to storable renewable energy in the form of chemical bonds, requires optimization of a photoelectrochemical device based on photovoltaic tandem heterojunctions. We report a monolithic photocathode device architecture that exhibits significantly reduced surface reflectivity, minimizing parasitic light absorption and reflection losses. A tailored multifunctional crystalline titania interphase layer acts as a corrosion protection layer, with favorable band alignment between the semiconductor conduction band and the energy level for water reduction, facilitating electron transport at the cathode–electrolyte interface. It also provides a favorable substrate for adhesion of high-activity Rh catalyst nanoparticles. Under simulated AM 1.5G irradiation, solar-to-hydrogen efficiencies of 19.3 and 18.5% are obtained in acidic and neutral electrolytes, respectively. The system reaches a value of 0.85 of the theoretical limit for photoelectrochemical water splitting for the energy gap combination employed in the tandem-junction photoelectrode structure.
quote
| GB/T 7714-2015 | [1] WenHui Cheng, Matthias H. Richter, Matthias M. May, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b00920. |
| MLA | [1] WenHui Cheng, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b00920. |
| APA | [1] WenHui Cheng, Matthias H. Richter, Matthias M. May, Jens Ohlmann, David Lackner, Frank Dimroth, Thomas Hannappel, Harry A. Atwater, & HansJoachim Lewerenz. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b00920 |
| IEEE | [1] WenHui Cheng, Matthias H. Richter, Matthias M. May, Jens Ohlmann, David Lackner, Frank Dimroth, Thomas Hannappel, Harry A. Atwater, and HansJoachim Lewerenz, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b00920. |