Weak Solvent–Solvent Interaction Enables High Stability of Battery Electrolyte AITranslate

China|University of Science and Technology of China; King Abdullah University of Science and Technology; Changchun Institute of Applied Chemistry; Changchun Institute of Applied Chemistry; Changchun Institute of Applied Chemistry; Changchun Institute of Applied Chemistry; King Abdullah University of Science and Technology; Changchun Institute of Applied Chemistry; China|University of Science and Technology of China
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Electrolytes play an important role in transporting metal ions (e.g., Li+) in metal ion batteries, while understanding the relationship between the electrolyte properties and behaviors is still challenging. Herein, we detect the existence of weak solvent–solvent interactions in electrolytes by nuclear magnetic resonance (NMR), particularly discovering that such interactions have a significant function of stabilizing the electrolytes, which has never been reported before. As a paradigm, we renovated the understanding of the role of ethylene carbonate (EC) solvent in the lithium-ion battery electrolyte. We find that the EC solvent can stabilize the linear carbonate solvent electrolyte, particularly the diethyl carbonate (DEC) electrolyte, by the weak intermolecular interactions, enhancing the energy difference between the orbitals of the Li+(EC)x(DEC)y complex, in turn demonstrating strong capability against reduction. Our viewpoint was further demonstrated in other metal ion batteries (e.g., Na+, K+), whose discovery is significant for designing electrolytes and in-depth understanding of the battery performance.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c00052

Chinese Library Classification Number:

Citation Information:

Electrolytes play an important role in transporting metal ions (e.g., Li+) in metal ion batteries, while understanding the relationship between the electrolyte properties and behaviors is still challenging. Herein, we detect the existence of weak solvent–solvent interactions in electrolytes by nuclear magnetic resonance (NMR), particularly discovering that such interactions have a significant function of stabilizing the electrolytes, which has never been reported before. As a paradigm, we renovated the understanding of the role of ethylene carbonate (EC) solvent in the lithium-ion battery electrolyte. We find that the EC solvent can stabilize the linear carbonate solvent electrolyte, particularly the diethyl carbonate (DEC) electrolyte, by the weak intermolecular interactions, enhancing the energy difference between the orbitals of the Li+(EC)x(DEC)y complex, in turn demonstrating strong capability against reduction. Our viewpoint was further demonstrated in other metal ion batteries (e.g., Na+, K+), whose discovery is significant for designing electrolytes and in-depth understanding of the battery performance.

quote

GB/T 7714-2015 [1] Yuqi Wang, Zhen Cao, Zheng Ma, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c00052.
MLA [1] Yuqi Wang, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c00052.
APA [1] Yuqi Wang, Zhen Cao, Zheng Ma, Gang Liu, Haoran Cheng, Yeguo Zou, Luigi Cavallo, Qian Li, & Jun Ming. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c00052
IEEE [1] Yuqi Wang, Zhen Cao, Zheng Ma, Gang Liu, Haoran Cheng, Yeguo Zou, Luigi Cavallo, Qian Li, and Jun Ming, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c00052.