daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Solvent-Free and Long-Cycling Garnet-Based Lithium-Metal Batteries AITranslate

ShanghaiTech University; ShanghaiTech University; ShanghaiTech University; ShanghaiTech University; ShanghaiTech University; ShanghaiTech University; ShanghaiTech University; ShanghaiTech University; ShanghaiTech University; ShanghaiTech University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Solid-state batteries using ceramic solid electrolytes promise to deliver enhanced energy density and intrinsic safety. However, the challenge of integrating solid electrolytes with electrode materials limits the electrochemical performance. Herein, we report a solvent-free ceramic-based lithium-metal battery with good cycling stability at a wide temperature range from 45 to 100 °C, enabled by an inorganic ternary salt of low eutectic point. By using a garnet electrolyte with molten salts at the electrolyte|cathode interface, the Li||LiFePO4 cells perform a long cycling with capacity retention of 81.4% after 1000 cycles at 1 C. High-voltage LiFe0.4Mn0.6PO4 cathodes also deliver good electrochemical performance. Specifically, commercial electrode pieces with high area capacities can be adopted directly in the quasi-solid-state lithium-metal batteries. These stable performances are ascribable to the low melting point, high ionic conductivity and good thermal/electrochemical stability of the ternary salt system. Our findings provide an effective method on fabrication of solid-state batteries for practical applications.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c00088

Chinese Library Classification Number:

Citation Information:

Solid-state batteries using ceramic solid electrolytes promise to deliver enhanced energy density and intrinsic safety. However, the challenge of integrating solid electrolytes with electrode materials limits the electrochemical performance. Herein, we report a solvent-free ceramic-based lithium-metal battery with good cycling stability at a wide temperature range from 45 to 100 °C, enabled by an inorganic ternary salt of low eutectic point. By using a garnet electrolyte with molten salts at the electrolyte|cathode interface, the Li||LiFePO4 cells perform a long cycling with capacity retention of 81.4% after 1000 cycles at 1 C. High-voltage LiFe0.4Mn0.6PO4 cathodes also deliver good electrochemical performance. Specifically, commercial electrode pieces with high area capacities can be adopted directly in the quasi-solid-state lithium-metal batteries. These stable performances are ascribable to the low melting point, high ionic conductivity and good thermal/electrochemical stability of the ternary salt system. Our findings provide an effective method on fabrication of solid-state batteries for practical applications.

quote

GB/T 7714-2015 [1] Jiameng Yu, Wenbo Zhai, Chang Zhang, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c00088.
MLA [1] Jiameng Yu, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c00088.
APA [1] Jiameng Yu, Wenbo Zhai, Chang Zhang, Cong Wu, Ran Wei, Shaojie Chen, Yingjie He, Qilin Hu, Yi Yu, & Wei Liu. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c00088
IEEE [1] Jiameng Yu, Wenbo Zhai, Chang Zhang, Cong Wu, Ran Wei, Shaojie Chen, Yingjie He, Qilin Hu, Yi Yu, and Wei Liu, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c00088.