Charge-Carrier Dynamics of Solution-Processed Antimony- and Bismuth-Based Chalcogenide Thin Films AITranslate

Wuhan University; University of Oxford; Wuhan University; University of Oxford; Wuhan University; Wuhan University; Wuhan University; Wuhan University; Wuhan University; Wuhan University; University of Oxford; Technical University of Munich; Wuhan University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Chalcogenide-based semiconductors have recently emerged as promising candidates for optoelectronic devices, benefiting from their low-cost, solution processability, excellent stability and tunable optoelectronic properties. However, the understanding of their fundamental optoelectronic properties is far behind the success of device performance and starts to limit their further development. To fill this gap, we conduct a comparative study of chalcogenide absorbers across a wide material space, in order to assess their suitability for different types of applications. We utilize optical-pump terahertz-probe spectroscopy and time-resolved microwave conductivity techniques to fully analyze their charge-carrier dynamics. We show that antimony-based chalcogenide thin films exhibit relatively low charge-carrier mobilities and short lifetimes, compared with bismuth-based chalcogenides. In particular, AgBiS2 thin films possess the highest mobility, and Sb2S3 thin films have less energetic disorder, which are beneficial for photovoltaic devices. On the contrary, Bi2S3 showed ultralong carrier lifetime and high photoconductive gain, which is beneficial for designing photoconductors.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c00140

Chinese Library Classification Number:

Citation Information:

Chalcogenide-based semiconductors have recently emerged as promising candidates for optoelectronic devices, benefiting from their low-cost, solution processability, excellent stability and tunable optoelectronic properties. However, the understanding of their fundamental optoelectronic properties is far behind the success of device performance and starts to limit their further development. To fill this gap, we conduct a comparative study of chalcogenide absorbers across a wide material space, in order to assess their suitability for different types of applications. We utilize optical-pump terahertz-probe spectroscopy and time-resolved microwave conductivity techniques to fully analyze their charge-carrier dynamics. We show that antimony-based chalcogenide thin films exhibit relatively low charge-carrier mobilities and short lifetimes, compared with bismuth-based chalcogenides. In particular, AgBiS2 thin films possess the highest mobility, and Sb2S3 thin films have less energetic disorder, which are beneficial for photovoltaic devices. On the contrary, Bi2S3 showed ultralong carrier lifetime and high photoconductive gain, which is beneficial for designing photoconductors.

quote

GB/T 7714-2015 [1] Zhenglin Jia, Marcello Righetto, Yujie Yang, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c00140.
MLA [1] Zhenglin Jia, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c00140.
APA [1] Zhenglin Jia, Marcello Righetto, Yujie Yang, Chelsea Q. Xia, Yanyan Li, Ruiming Li, Yuwei Li, Bin Yu, Yong Liu, Huiming Huang, Michael B. Johnston, Laura M. Herz, & Qianqian Lin. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c00140
IEEE [1] Zhenglin Jia, Marcello Righetto, Yujie Yang, Chelsea Q. Xia, Yanyan Li, Ruiming Li, Yuwei Li, Bin Yu, Yong Liu, Huiming Huang, Michael B. Johnston, Laura M. Herz, and Qianqian Lin, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c00140.