daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone qikanliebiao
Article List
Browse all articles published in this journal

Study of Ga Recovery from Granulation Slag

Rare Metals and Cemented Carbides | Vol., Issue 1, 2003 | pp. 8-10
Study is made of Ga recovery process from ISP or fuming furnace granulation slag.Ga is extracted from H2SO4 medium with N1923 as extractant by a unique leaching technology of enriched H2SO4 at constant temperature and elimination of Si impact on liquid-solid separation.The enriched product with Ga assaying 2.82% is obtained.
DOI: Cited: 0 Download: 0

Study of Ultra-fine WC Powder Preparation by Mechanical Ball Milling

Rare Metals and Cemented Carbides | Vol., Issue 1, 2003 | pp. 11-14
Study is made of the vibrating ball miling for ultra-fine WC powder preparation.Coarse,medium and fine WC powders are used for tests at different ball percentage and milling time.The results showed that longer ball milling time cam result in ultra-fine WC powder with FSSS particale size<0.5 μm,while larger ball percentage and longer milling tine can make the particle size smaller yet without any influence on the particle size distribution.The milled powder size distribution is related to that of the primary powder.The longer milling time will result in smaller grain size and larger stress.
DOI: Cited: 0 Download: 0

The Study on a New Technique of W powder Blending With Carbon for Hard-alloy Production

Rare Metals and Cemented Carbides | Vol., Issue 1, 2003 | pp. 15-17
Description is made of a new technique for hard alloy production by a new process of W powder directly blending with carbon without carbonization.Through preliminary exploration,hard alloys with ideal property are obtained.The author believes that this process is characterized by low operating cost,good product quality,being easy to popularize.It is worthwhile to be further improved and made perfect.
DOI: Cited: 0 Download: 0

Investigation and Practice of Serial Column Absorption and Stripping Process for W ion Exchange

Rare Metals and Cemented Carbides | Vol., Issue 1, 2003 | pp. 20-21
Brief description is made of the new process of serial column absorption and stripping for W ion exchange.It is pointed out that under the same condition,the new process will result in about 100mg/g(dry resin) more W absorption (as WO3) and 80 g/L more WO3 in the stripped peak solution than that by the original process with lower impurity element content in the solution,resulting in better-quality APT. APT yield increased about 15 g/L than the original process as well as~10% reduction of ammonium chloride consumption,indicating distinct economic returns from the new process.
DOI: Cited: 0 Download: 0

Preparation and Application of Nanometer TiO_2

Rare Metals and Cemented Carbides | Vol., Issue 1, 2003 | pp. 25-27
The paper has reviewed Nanorneter TiO2 preparation methods and its advantages and disadvantages are compared.The paper describes its current applications in the fields of light catalyst,environmental protection,cosmetics and wave absorption mat erials.It also pointed out the problems to be solved in the course of Nanometer TiO2 preparation.
DOI: Cited: 0 Download: 0