Adsorption Behavior of Chelate Resin for Vanadium(Ⅳ) Ion AITranslate
Abstract AITranslate
The adsorption behavior of chelate resin A for vanadium (Ⅳ) ion was studied,and the effects of acidity, resin dosage, reaction time and temperature and concentration of the standard vanadium solution on static adsorption were investigated. The results show that chelate resin A can adsorb 184.2 mg/g vanadium (Ⅳ) under the conditions of pH4,1.0 g resin, 60 ℃× 4 h reaction. In addition, desorption behavior of the chelate resin and effect of coexisting cations were analyzed.
KeyWords AITranslate
1陆芝华,周邦娜,余仲兴,陈世.石煤氧化焙烧-稀碱溶液浸出提钒工艺研究[J].稀有金属,1994,18(5):321-327. 被引量:24
2高玉敏.亚铁容量法测定钒渣中的钒量[J].铁合金,2003,34(3):44-46. 被引量:7
3熊春华,莫建军,林峰.铀酰离子在大孔膦酸树脂上的吸附行为及其机理[J].铀矿冶,1994,13(4):264-267. 被引量:17
4李晓健.酸浸-萃取工艺在石煤提钒工业中的设计与应用[J].湖南有色金属,2000,16(3):21-23. 被引量:44
5王先良,王小利,徐顺清.大孔螯合树脂可用于处理中药重金属污染[J].中成药,2005,27(12):1376-1379. 被引量:43
1杨小慧,李望,朱晓波.D751螯合树脂吸附酸性溶液中钒(Ⅳ)离子的机制[J].中国有色金属学报,2022,32(12):3862-3870.
1刘树惠.碳还原后的氧化轨中钒(Ⅲ)钒(Ⅳ)钒(Ⅴ)的测定[J].钢铁钒钛,1989,10(4):67-70. 被引量:2
2Б.,ЛХ,国强.用二—2—乙基己基磷酸从硫酸溶液中萃取钒(Ⅳ)的动力学[J].钒钛,1990(4):3-5.
3曾小明,黄慧敏,司士辉.C-900氨基膦酸树脂对钒(Ⅳ)离子的吸附行为研究[J].稀有金属与硬质合金,2012,40(2):6-9. 被引量:6
4Ipin.,KO,许孙曲.在化学动力学控制区内萃取钒(Ⅳ)的机理[J].钒钛,1991(3):10-13. 被引量:1
5陈兴龙,朱火清,吴海鹰,李桂英,吴美斌,刘天平.皂化P_(204)微乳液膜萃取分离钒铁的研究[J].材料研究与应用,2008,2(2):137-140. 被引量:10
6G.V.Ramana Murthy,游建南.用2-羟苯乙酮肟萃取和同时分光光度测定混合物中钒(Ⅳ)和钒(Ⅴ)[J].湿法冶金,1990(2):80-83.
7王劲松,曹诗倜.用4,5—二溴苯基荧光酮分光光度法测定痕量钒[J].湖南冶金,1993(6):33-35.
8肖新望,刘绍书,熊平.用树脂矿浆法从石煤中提取钒[J].湿法冶金,2007,26(2):84-87. 被引量:11
9田宇红,兰新哲,孙小刚,陈向阳.树脂吸附法去除尾矿浆中氰化物的研究[J].湿法冶金,2010,29(1):49-51. 被引量:1
10修慧敏,徐斌,徐小卫,沈建华.用离子交换法分离钼酸铵溶液中的钒[J].湿法冶金,2010,29(4):267-269. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TF841.3[冶金工程—有色金属冶金]
Citation Information:
The adsorption behavior of chelate resin A for vanadium (Ⅳ) ion was studied,and the effects of acidity, resin dosage, reaction time and temperature and concentration of the standard vanadium solution on static adsorption were investigated. The results show that chelate resin A can adsorb 184.2 mg/g vanadium (Ⅳ) under the conditions of pH4,1.0 g resin, 60 ℃× 4 h reaction. In addition, desorption behavior of the chelate resin and effect of coexisting cations were analyzed.
quote
| GB/T 7714-2015 | [1] HUANG Hui-min, CHEN Hui, SI Shi-hui, et al. Adsorption Behavior of Chelate Resin for Vanadium(Ⅳ) Ion[J]. Rare Metals and Cemented Carbides, 2012(1): 18-20. |
| MLA | [1] HUANG Hui-min, et al., "Adsorption Behavior of Chelate Resin for Vanadium(Ⅳ) Ion." Rare Metals and Cemented Carbides, no. 1, 2012, pp. 18-20. |
| APA | [1] HUANG Hui-min, CHEN Hui, SI Shi-hui, & DENG Chun-yan. (2012). Adsorption Behavior of Chelate Resin for Vanadium(Ⅳ) Ion. Rare Metals and Cemented Carbides(1), 18-20. |
| IEEE | [1] HUANG Hui-min, CHEN Hui, SI Shi-hui, and DENG Chun-yan, "Adsorption Behavior of Chelate Resin for Vanadium(Ⅳ) Ion," Rare Metals and Cemented Carbides, no. 1, pp. 18-20, 2012. keywords: {chelate resin A;adsorption behavior;vanadium ( Ⅳ) ion} |