Abstract AITranslate
Monoclinic MnOOH nanotubes were synthesized for the first time by oxidizing the self-sacrificing template of β-MnO2 nanotubes in stainless steel autoclave at 200℃ for 48 h. The prepared samples were characterized by XRD,TEM,SAED,FESEM, HRTEM and EDS. The results show that the samples are pure single-crystal MnOOH nanotubes,having the diameters of 200-500 nm and the lengths of several microns.
KeyWords AITranslate
1董喜燕,张兴堂,程纲,李蕴才,杜祖亮.MnOOH纳米棒的反胶束法制备及表征[J].化学学报,2004,62(24):2441-2443. 被引量:14
2王莉,袁中直,陈秋红,孙峰,朱立才.方形γ-MnOOH单晶的水热法制备[J].无机材料学报,2007,22(4):667-670. 被引量:5
3张元广,陈友存.MnOOH纳米棒的低温水热合成[J].无机材料学报,2006,21(5):1249-1252. 被引量:5
4糜裕宏,张孝彬,周胜名,王杏花,贺狄龙,王俊莲.多枝状γ-MnOOH的低温水热合成与表征[J].无机化学学报,2006,22(12):2242-2246. 被引量:3
1陈琳,田俐,李帅,朱金良,吕数子.溶剂热法制备纳米MnOOH[J].化学研究,2011,22(1):53-57.
2朱刚,李树娜,李学坤.MnOOH结构,制备方法和应用的研究进展[J].人工晶体学报,2018,47(1):166-171.
1杨尔慧,王俊勃,姜凤阳,思芳.牺牲模板法制备多孔陶瓷材料的研究进展[J].电子元件与材料,2015,34(8):5-8. 被引量:3
2周阿洋,郝建文,袁新松,周涛.自牺牲模板法制备氢氧化镁纳米棒[J].河南化工,2009,26(2):14-16.
3李中春,顾爱军,周全法.简单水热法合成MnOOH纳米棒及应用(英文)[J].稀有金属材料与工程,2016,45(4):863-868. 被引量:2
4臭氧氧化法制备二氧化锰[J].无机盐工业,2011,43(7):28-28.
5董喜燕,张兴堂,程纲,李蕴才,杜祖亮.MnOOH纳米棒的反胶束法制备及表征[J].化学学报,2004,62(24):2441-2443. 被引量:14
6仝源.不锈钢反应釜螺旋半管修补[J].石油化工设备,2010,39(1):90-92.
7夏熙.二氧化锰的物理、化学性质与其电化学活性的相关(4)[J].电池,2006,36(3):195-198. 被引量:6
8王东光,竺柏康,陶亨聪.高频率撞击流反应器制备Fe_3O_4/MnOOH核壳纳米颗粒(英文)[J].中国化学工程学报:英文版,2015,23(4):727-735. 被引量:1
9李小红,古训玖,江向平,陈超,涂娜.纳米β-MnO_2空心球的可控制备及其催化性能研究[J].中国陶瓷,2010,46(10):16-18. 被引量:1
10胡扬剑,唐文琳.纺锤形MnO_2微晶的水热法制备[J].广东化工,2012,39(10):16-16.
Basic Information:
DOI:
Chinese Library Classification Number:TQ137.12[化学工程—无机化工]
Citation Information:
Monoclinic MnOOH nanotubes were synthesized for the first time by oxidizing the self-sacrificing template of β-MnO2 nanotubes in stainless steel autoclave at 200℃ for 48 h. The prepared samples were characterized by XRD,TEM,SAED,FESEM, HRTEM and EDS. The results show that the samples are pure single-crystal MnOOH nanotubes,having the diameters of 200-500 nm and the lengths of several microns.
quote
| GB/T 7714-2015 | [1] YANG Bao-jun, ZHOU Tao, ZHOU A-yang. Research on Synthesizing MnOOH Nanotubes with Self-sacrificing Template Route[J]. Rare Metals and Cemented Carbides, 2009(3): 1-4. |
| MLA | [1] YANG Bao-jun, et al., "Research on Synthesizing MnOOH Nanotubes with Self-sacrificing Template Route." Rare Metals and Cemented Carbides, no. 3, 2009, pp. 1-4. |
| APA | [1] YANG Bao-jun, ZHOU Tao, & ZHOU A-yang. (2009). Research on Synthesizing MnOOH Nanotubes with Self-sacrificing Template Route. Rare Metals and Cemented Carbides(3), 1-4. |
| IEEE | [1] YANG Bao-jun, ZHOU Tao, and ZHOU A-yang, "Research on Synthesizing MnOOH Nanotubes with Self-sacrificing Template Route," Rare Metals and Cemented Carbides, no. 3, pp. 1-4, 2009. keywords: {MnOOH;nanotube;monoclinic phase;β-MnO2;self-sacrificing template} |