Study on the New Process of Vanadium Extraction from Siliceous Stone Coal AITranslate
Abstract AITranslate
Based on the single-factor condition test,the optimal technological parameters are determined for vanadium extraction by the"roasting without additives-alkaline leaching"and the oxidizer-oxidizing-acid leaching processes.The test results show that with mineral particle size 0.074 mm,oxygen partial pressure 10~100 Pa,roasting duration 3 h,leaching temperature 90 ℃,3 h leaching duration,caustic soda concentration 40 g/L,liquid-solid ratio 1.5∶1.0,the leaching rate of vanadium pentoxide by roasting without additives-alkaline leaching" can reach 83.8%,20% higher than that bytraditional sodium roasting-acid or alkaline leaching,with mineral particle size 0.074 mm,MnO2 oxidizer consumption at 5%,sulfuric acid concentration at 40%,leaching temperature 90 ℃,9 h leaching duration,liquid-solid ratio 2.5∶1.0,the leaching rate of vanadium pentoxide by oxidizer-oxidizing-acid leaching can reach 72.4%,10% higher than that by the traditional sodium roasting.
KeyWords AITranslate
1蔡晋强,巴陵.石煤提钒的几种新工艺[J].矿产保护与利用,1993(5):30-33. 被引量:21
2钱强.石煤钒矿提取五氧化二钒的技术现状[J].中国资源综合利用,2008,26(3):13-14. 被引量:17
3张萍,蒋馥华.苛化泥为焙烧添加剂从石煤提取五氧化二钒[J].稀有金属,2000,24(2):115-118. 被引量:15
4谭爱华.某石煤钒矿空白焙烧-碱浸提钒工艺研究[J].湖南有色金属,2008,24(1):24-26. 被引量:34
5梁江龙,方正,李浩然,冯雅丽.酸浸法从黏土钒矿中提钒[J].有色金属,2008,60(1):80-82. 被引量:17
1毛益林,陈晓青,杨进忠,王秀芬.陕西某低品位粘土钒矿选矿富集工艺研究[J].矿冶工程,2016,36(3):44-46. 被引量:4
2尹飞,邹维,揭晓武,张永禄,王振文.高硅质石煤钒矿浸出机理研究[J].有色金属:冶炼部分,2016(9):21-23. 被引量:4
3蹇兴文,黄晶,张一敏,蔡震雷,刘红.氢氧化钠碱熔焙烧对页岩提钒过程的影响[J].有色金属:冶炼部分,2018(3):30-34. 被引量:2
4汪忠良.陕西商洛黏土型钒矿焙烧提钒工艺研究[J].中国金属通报,2020(6):6-7.
1胡洋,何东升,谢志豪,吴玉元,李克尧.石煤型钒矿预富集技术研究现状[J].金属矿山,2018,47(12):73-79. 被引量:14
2朱一民,周菁.2016年浮选药剂的进展[J].矿产综合利用,2017(3):1-16. 被引量:2
3邹建新.钒渣浸出过程的热力学和动力学研究现状[J].无机盐工业,2018,50(12):5-8.
4卜浩,吕昊子,曹苗,高玉德,何名飞,孟庆波,李双棵.废SCR脱硝催化剂钒钨提取研究进展[J].有色金属:冶炼部分,2020,0(5):79-85. 被引量:3
5汪忠良.陕西商洛黏土型钒矿焙烧提钒工艺研究[J].中国金属通报,2020(6):6-7.
6袁杰,李松,肖劲.响应曲面法优化铝电解废阴极碱熔提纯工艺[J].有色金属:冶炼部分,2020(9):120-126. 被引量:5
7包申旭,陈波,张一敏.我国钒页岩提钒技术研究现状及前景[J].金属矿山,2020(10):20-33. 被引量:8
8朱军,康敏,李维亮,王斌,齐建云,李姝,刘丹阳.粘土钒矿钡盐焙烧-酸浸提钒工艺研究[J].材料导报,2020,34(24):24061-24067. 被引量:1
9田宗平,彭君,王干珍,易晓明,曹健,秦毅.石煤钒矿成分分析标准物质的研制[J].岩矿测试,2021,40(1):111-120. 被引量:5
10王振文,尹飞,邹维,江培海,阮书峰.石煤硫酸浸出过程中含钒矿物的浸出行为[J].有色金属工程,2023,13(4):45-54.
1朱靖,刘永光,王岭.钒提取工艺研究进展[J].现代矿业,2011(6):122-123. 被引量:5
2许国镇.石煤中钒的价态及物质组成对提钒工艺的指导作用[J].煤炭加工与综合利用,1989(5):5-8. 被引量:48
3任泽民,刘代俊.电渗析法处理碱法提钒浸出液[J].应用化工,2012,41(2):214-216. 被引量:1
4杨静翎,金鑫.酸浸法提钒新工艺的研究[J].北京化工大学学报:自然科学版,2007,34(3):254-257. 被引量:40
5韦斌,傅晓恒,王龙龙,张静波,李福俊.赤泥硫酸浸出金属钛实验的动力学研究[J].世界科技研究与发展,2008,30(6):697-699. 被引量:11
6汪超,吴封,韦林森,邓孝伯.带式过滤机在水浸提钒工艺中的应用[J].过滤与分离,2015,25(2):24-26. 被引量:3
7潘占开,李青春,叶树峰,钱鹏,何海兴,殷保稳.方山口石煤钒矿空白焙烧——助浸剂浸出工艺研究[J].计算机与应用化学,2014,31(12):1557-1560. 被引量:5
8严健.烧碱浓度的测量及测温点的选择[J].江苏氯碱,1991(4):21-22.
9谢炳俊,纪律,陈高琪,孙进贺,贾永忠.正浮选工艺矿物粒度对氯化钾分布的影响[J].无机盐工业,2014,46(12):38-40. 被引量:6
10焦向科,张一敏,陈铁军.高硅钒尾矿作水泥混合材的试验研究[J].新型建筑材料,2012,39(9):4-6. 被引量:10
Basic Information:
DOI:
Chinese Library Classification Number:TQ135.11[化学工程—无机化工]
Citation Information:
Based on the single-factor condition test,the optimal technological parameters are determined for vanadium extraction by the"roasting without additives-alkaline leaching"and the oxidizer-oxidizing-acid leaching processes.The test results show that with mineral particle size 0.074 mm,oxygen partial pressure 10~100 Pa,roasting duration 3 h,leaching temperature 90 ℃,3 h leaching duration,caustic soda concentration 40 g/L,liquid-solid ratio 1.5∶1.0,the leaching rate of vanadium pentoxide by roasting without additives-alkaline leaching" can reach 83.8%,20% higher than that bytraditional sodium roasting-acid or alkaline leaching,with mineral particle size 0.074 mm,MnO2 oxidizer consumption at 5%,sulfuric acid concentration at 40%,leaching temperature 90 ℃,9 h leaching duration,liquid-solid ratio 2.5∶1.0,the leaching rate of vanadium pentoxide by oxidizer-oxidizing-acid leaching can reach 72.4%,10% higher than that by the traditional sodium roasting.
quote
| GB/T 7714-2015 | [1] SUN De-si, ZHANG Li-ming, ZHANG Xian-zhen. Study on the New Process of Vanadium Extraction from Siliceous Stone Coal[J]. Rare Metals and Cemented Carbides, 2010(2): 5-10. |
| MLA | [1] SUN De-si, et al., "Study on the New Process of Vanadium Extraction from Siliceous Stone Coal." Rare Metals and Cemented Carbides, no. 2, 2010, pp. 5-10. |
| APA | [1] SUN De-si, ZHANG Li-ming, & ZHANG Xian-zhen. (2010). Study on the New Process of Vanadium Extraction from Siliceous Stone Coal. Rare Metals and Cemented Carbides(2), 5-10. |
| IEEE | [1] SUN De-si, ZHANG Li-ming, and ZHANG Xian-zhen, "Study on the New Process of Vanadium Extraction from Siliceous Stone Coal," Rare Metals and Cemented Carbides, no. 2, pp. 5-10, 2010. keywords: {siliceous stone coal;roasting without additive;alkaline leaching;oxidizer;acid leaching;vanadium extraction process} |