Analysis of Extraction Mechanism and Extraction Equilibrium Constant of La in P204-HCl-HAc System AITranslate

Liaoning University of Petroleum and Chemical Technology;Liaoning University of Petroleum and Chemical Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

At pH1,La concentration is determined by EDTA volumetric titration in the two phases of P204-HCl-HAc extraction system,and study is made on the effect of solution acidity and extractant concentration on La distribution ratio.Based on the infrared spectrum testing and analysis of La loaded organic phase in the P204-HCl-HAc system,investigation is made on the extraction mechanism of La in P204-HCl-HAc system and the extraction equilibrium constant is determined.The results show that at pH1,the extraction is actually a displacement reaction between La and group P-OH based on the cation exchange mechanism and complexing and coordination action between La and group P=O with extraction equilibrium constant KLa is 10-0.02.

KeyWords AITranslate

P204-HCl-Hac lainfrared spectrum extraction mechanism extraction equilibrium constant

1沈玉华,王笃金,吴瑾光.D2EHPA萃取稀土的有机相红外光谱及添加DMHPA的影响[J].光谱学与光谱分析,1997,17(3):32-35. 被引量:7

2单欣昌,秦炜,戴猷元.萃取剂相对酸(碱)度对极性有机物络合萃取平衡的影响[J].高校化学工程学报,2005,19(5):593-597. 被引量:9

3孙盈,李艳玲,权新军,廖伍平.二-(2-乙基己基)磷酸P204与三烷基叔胺N235协同萃取钼[J].应用化学,2009,26(11):1353-1356. 被引量:11

4沈玉华,谢安建,廖旭华.不同萃取剂对含Ni(Ⅱ)有机相微结构的影响[J].中国科学技术大学学报,1998,28(2):252-256. 被引量:6

5刘建,李建.P_(204)-kerosene-EDTA体系萃取分离钨钼[J].中国钼业,2007,31(4):26-29. 被引量:10

6付子忠,郑剑平,赵瑞卿,付晋.用草酸溶液从负载稀土的P204中直接反萃取沉淀稀土[J].湿法冶金,2000,19(4):6-11. 被引量:9

7常宏涛,吴文远,王丹,边雪,涂赣峰.P204-HCl-H_3cit体系中镧铈分配比及分离系数研究[J].稀有金属与硬质合金,2008,36(2):1-5. 被引量:4

1徐志高,王力军,吴延科,池汝安,李攀红,阳慧芳.DIBK-P204体系萃取分离锆和铪的机理[J].中国有色金属学报,2013,23(7):2061-2068. 被引量:10

1徐志高,李攀红,池汝安,王力军,吴明,赵骏.DIBK协萃体系负载有机相反萃行为研究[J].有色金属:冶炼部分,2015(4):20-23. 被引量:4

2董雪平,郭树军,徐欣.锆铪萃取分离机理的研究进展[J].广州化工,2015,43(23):42-44. 被引量:3

3李洁,王占明.电感耦合等离子体原子发射光谱法测定铪合金中锆[J].冶金分析,2016,36(1):71-74. 被引量:9

4李攀红,徐志高,池汝安,赵骏,王力军,徐源来.湿法分离锆铪的研究进展[J].稀有金属,2016,40(5):499-508. 被引量:8

5赵骏,徐志高,张文杰,李攀红,池汝安,徐源来.DIBK-TOPO体系萃取锆和铪的动力学研究[J].稀有金属,2017,41(1):108-112. 被引量:6

6柴延全,郑仕鸿,赵卓.锆铪分离技术的研究现状及发展趋势[J].有色金属工程,2017,7(2):30-34. 被引量:9

7王俊莲,付家帅,许文,王化军.基于锆铪溶剂萃取分离的萃取剂性能[J].稀有金属,2020,44(6):658-667. 被引量:7

8徐志高,徐斐,董攀飞,吴明,何正艳,瞿军,池汝安.溶剂协同萃取分离锆和铪技术研究进展[J].有色金属工程,2021,11(12):57-67.

9梁耕宇,苏学斌,刘康,王桂硕,程浩,张承天,刘忠臣,刘会武,向秋林.用N235从独居石优溶渣浸出液中萃取铁的动力学研究[J].湿法冶金,2023,42(2):127-132.

10刘辉,王化军,许文,徐国栋,刘璐,王俊莲.核级锆铪溶剂萃取分离研究进展[J].中国材料进展,2023,42(4):335-342.

1李剑虹.D_2EHPA-HCl-HAc体系萃取P_m(Ⅲ)的机理与平衡常数[J].有色金属:冶炼部分,2010(5):40-42.

2李剑虹.D_2 EHPA-HCl-HAc体系萃取Nd(Ⅲ)的机理分析与萃取平衡常数[J].矿冶,2011,20(1):43-46.

3许绍权,李素清,洪海玲.氟硅酸体系中D_2EHPA对铟和锡的非平衡萃取[J].稀有金属,1995,19(1):1-5. 被引量:7

4李素清,许绍权.黄金工艺与化学[J].化学世界,1994,35(5):235-238. 被引量:2

5伍志春,于淑秋.HEHEHP从硫酸盐溶液中萃取铁[J].化工冶金,1992,13(4):313-317. 被引量:3

6肖强.连铸坯的凝固与传热过程研究[J].中国新技术新产品,2012(19):170-170.

7张秀英,尹国寅,薄其兵.环烷酸/正庚烷萃取钪的机理研究[J].稀土,2001,22(2):14-16. 被引量:2

8肖彩林,朱鹄,吴家泉.碳糊电极阳极溶出伏安法用于高冰镍中Ni_3S_2相测定的研究[J].湖南有色金属,1990,0(1):44-46.

9罗金凤,胡立舜,丁英萍,邱祖民.从铋冶炼浸渣制取三盐基硫酸铅的研究[J].计算机与应用化学,2006,23(10):967-970.

10李连福,姜茂发.底吹电弧炉水模型熔池内气液综合传质系数的测定[J].东北大学学报:自然科学版,1996,17(5):480-484. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:TF845.6[冶金工程—有色金属冶金]

Citation Information:

At pH1,La concentration is determined by EDTA volumetric titration in the two phases of P204-HCl-HAc extraction system,and study is made on the effect of solution acidity and extractant concentration on La distribution ratio.Based on the infrared spectrum testing and analysis of La loaded organic phase in the P204-HCl-HAc system,investigation is made on the extraction mechanism of La in P204-HCl-HAc system and the extraction equilibrium constant is determined.The results show that at pH1,the extraction is actually a displacement reaction between La and group P-OH based on the cation exchange mechanism and complexing and coordination action between La and group P=O with extraction equilibrium constant KLa is 10-0.02.

quote

GB/T 7714-2015 [1] LI Jian-hong, ZHANG Xing. Analysis of Extraction Mechanism and Extraction Equilibrium Constant of La in P204-HCl-HAc System[J]. Rare Metals and Cemented Carbides, 2010(2): 11-13.
MLA [1] LI Jian-hong, and ZHANG Xing. "Analysis of Extraction Mechanism and Extraction Equilibrium Constant of La in P204-HCl-HAc System." Rare Metals and Cemented Carbides, no. 2, 2010, pp. 11-13.
APA [1] LI Jian-hong, & ZHANG Xing. (2010). Analysis of Extraction Mechanism and Extraction Equilibrium Constant of La in P204-HCl-HAc System. Rare Metals and Cemented Carbides(2), 11-13.
IEEE [1] LI Jian-hong and ZHANG Xing, "Analysis of Extraction Mechanism and Extraction Equilibrium Constant of La in P204-HCl-HAc System," Rare Metals and Cemented Carbides, no. 2, pp. 11-13, 2010. keywords: {P204-HCl-Hac;lainfrared spectrum;extraction mechanism;extraction equilibrium constant}