Effect of Annealing Temperature on Mechanical Properties of Zr-4 Alloy Different Diameter Pipe AITranslate

State Nuclear Power Titanium Zirconium Co., Ltd.;State Nuclear Power Titanium Zirconium Co., Ltd.;State Nuclear Power Titanium Zirconium Co., Ltd.;State Nuclear Power Titanium Zirconium Co., Ltd.;State Nuclear Power Titanium Zirconium Co., Ltd.;State Nuclear Power Titanium Zirconium Co., Ltd.;State Nuclear Power Titanium Zirconium Co., Ltd.;State Nuclear Power Titanium Zirconium Co., Ltd.
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The effect was investigated of annealing temperature on room temperature and high temperature mechanical properties of Zr-4alloy different diameter pipe with different deformation(50% and 18% retransformation after the first annealing).Metallurgical microstructure was observed by optical microscope of the alloy with 50% deformation and 18%retransformation after the first annealing at 523 ℃for 3.5h.The results show that room temperature mechanical properties of Zr-4alloy different diameter pipe with50% deformation depend on its first annealing temperature,and that of the pipe with 18%retransformation after its first annealing depend on its second annealing temperature.When Zr-4alloy different diameter pipe with 50% and 18%retransformation after its first annealing is annealed at 540℃for 3.5h,it has the maximum high temperature elongation.After twice 523℃/3.5hannealing,the pipe with 50% deformation has typical equiaxed microstructure with completely recrystallized morphology.After once 523℃/3.5hannealing,the pipe with 18% retransformation has the microstructure of vague and disordered morphology,and its grains still have strong directionality with the typical morphology in stress-relief state.

KeyWords AITranslate

Zr-4 alloy different diameter pipe annealing temperature mechanical property

1林金平,张军,祝国梁,王俊,郭有军,赵洪生,孙宝德.镓对Al-Mg-Si合金微观组织及拉伸性能的影响研究[J].材料工程,2009,37(S1):236-240. 被引量:1

2谈荣生,孙连超,刘心红,张毅.稀土对HSn70-1锡黄铜高温性能影响的研究[J].中国稀土学报,1995,13(S1):462-465. 被引量:3

3徐海林,董洪波,朱深亮,王志录,江斌.双重退火对TC21钛合金高温变形后组织的影响[J].材料热处理学报,2014,35(7):65-68. 被引量:6

4袁均平,易丹青,余志明,黄正成,吴伯涛,张霞.变形与热处理对Invar合金组织及性能的影响[J].金属热处理,2005,30(2):50-53. 被引量:12

5王春炎,曲文卿,姚君山,赵海云.2219-T87铝合金搅拌摩擦焊接头组织与力学性能[J].焊接学报,2010,31(10):77-80. 被引量:40

6张静,常永勤,贺建超,万发荣.氧化物弥散强化材料的搅拌摩擦焊分析[J].焊接学报,2015,36(7):63-66.

7姜庆伟,杨杰.二次退火对工业纯钛组织及性能的影响[J].钢铁钒钛,2016,37(1):37-40. 被引量:3

8黄德明,梁盛隆,唐静,杨雄飞,蒋仁贵.不同热处理制度下TC4合金棒材的组织与性能[J].钢铁钒钛,2014,35(5):25-30. 被引量:3

9雷喆,柳光祖,杨峥.MGH754合金冷轧板材的再结晶行为[J].钢铁研究学报,2013,25(5):49-53. 被引量:1

10惠希东,滕新营,王执福,王守仁.氮对0.3C-26Cr-8Ni耐热钢组织与性能的影响[J].特殊钢,1997,18(3):14-17. 被引量:4

Basic Information:

DOI:

Chinese Library Classification Number:TG166.7[金属学及工艺—热处理]

Citation Information:

The effect was investigated of annealing temperature on room temperature and high temperature mechanical properties of Zr-4alloy different diameter pipe with different deformation(50% and 18% retransformation after the first annealing).Metallurgical microstructure was observed by optical microscope of the alloy with 50% deformation and 18%retransformation after the first annealing at 523 ℃for 3.5h.The results show that room temperature mechanical properties of Zr-4alloy different diameter pipe with50% deformation depend on its first annealing temperature,and that of the pipe with 18%retransformation after its first annealing depend on its second annealing temperature.When Zr-4alloy different diameter pipe with 50% and 18%retransformation after its first annealing is annealed at 540℃for 3.5h,it has the maximum high temperature elongation.After twice 523℃/3.5hannealing,the pipe with 50% deformation has typical equiaxed microstructure with completely recrystallized morphology.After once 523℃/3.5hannealing,the pipe with 18% retransformation has the microstructure of vague and disordered morphology,and its grains still have strong directionality with the typical morphology in stress-relief state.

quote

GB/T 7714-2015 [1] YU Jun-hui, YUAN Gai-huan, WANG Zeng-min, et al. Effect of Annealing Temperature on Mechanical Properties of Zr-4 Alloy Different Diameter Pipe[J]. Rare Metals and Cemented Carbides, 2015(3): 46-49.
MLA [1] YU Jun-hui, et al., "Effect of Annealing Temperature on Mechanical Properties of Zr-4 Alloy Different Diameter Pipe." Rare Metals and Cemented Carbides, no. 3, 2015, pp. 46-49.
APA [1] YU Jun-hui, YUAN Gai-huan, WANG Zeng-min, JIANG You-rong, LV Liang-liang, YANG Hui, LIU Lei, & LI Qi-ming. (2015). Effect of Annealing Temperature on Mechanical Properties of Zr-4 Alloy Different Diameter Pipe. Rare Metals and Cemented Carbides(3), 46-49.
IEEE [1] YU Jun-hui, YUAN Gai-huan, WANG Zeng-min, JIANG You-rong, LV Liang-liang, YANG Hui, LIU Lei, and LI Qi-ming, "Effect of Annealing Temperature on Mechanical Properties of Zr-4 Alloy Different Diameter Pipe," Rare Metals and Cemented Carbides, no. 3, pp. 46-49, 2015. keywords: {Zr-4 alloy;different diameter pipe;annealing temperature;mechanical property}