daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Preparation of Pr Metal by Electrolysis of Pr Oxide Research and Industrial Practice AITranslate

Hunan Rare Earth Metal Materials Research Institute;Hunan Rare Earth Metal Materials Research Institute;Hunan Rare Earth Metal Materials Research Institute;Hunan Rare Earth Metal Materials Research Institute
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The paper briefly describes the bench scale test and 3 000 A electrolyzer pro duction of Pr metal by electrolysis of Pr oxide. The influence of electrolyte composition,electrolysis temperature, cathode current density and feedrate on the production efficiency is discussed. The practice shows that the electrolyzer has worked continuously and stably on a self-heating basis.The daily output of Pr metal per electrolyzer reached 65~70kg,metal re covery 90%,current efficiency>80%.

KeyWords AITranslate

electrolysis of Pr_6O11 Pr metal technology industrial practice

1王毅军.熔盐电解氧化钇制取Al-Y合金工艺的研究[J].稀有金属与硬质合金,1992,20(3):25-27. 被引量:4

2刘天明.关于稀土氧化物熔盐电解反应机理的探讨[J]稀有金属,1984(04).

1王毅军,舒斌,张跃.NdFeB磁性材料制造工业废料中金属钕的提炼[J].上海有色金属,2000,21(1):21-24. 被引量:3

2王毅军,舒斌,张跃.从NdFeB磁性材料制造工业废料中提炼金属钕[J].稀有金属与硬质合金,2000,28(1):48-52. 被引量:12

1张伟南,陈栋华.草酸盐在无机功能材料中的应用[J].中南民族大学学报:自然科学版,2004,23(2):29-32. 被引量:3

2李志强,李三喜.超细钛酸钡粉体湿化学合成技术[J].山东陶瓷,2004,27(5):14-17. 被引量:2

3陈早明,谢志鹏.超细钛酸钡粉体的制备方法[J].江西化工,2006(4):19-21.

4甘世宇,陈芳,古映莹,董兴镖,陈熙.湿化学法制备超细钛酸钡粉体的研究进展[J].材料导报,2007,21(F11):173-176. 被引量:5

5石爱华,颜文斌,李佑稷,张赞.苹果酸络合物沉淀法制备纳米二氧化钛粉体[J].中国粉体技术,2008,14(2):12-13.

6颜文斌,石爱华,覃事栋,李佑稷,周海洪.氨三乙酸盐沉淀法制备纳米钛酸钡粉体[J].稀有金属材料与工程,2008,37(A02):344-346.

7黄劲松,齐美富.钕铁硼废料资源化利用工艺综述[J].中国资源综合利用,2008,26(11):4-5. 被引量:12

8魏成富,代强,唐杰,杨梨容,李想,张林.硫酸复盐法回收NdFeB废料中含铁水的处理[J].绵阳师范学院学报,2010,29(5):38-40. 被引量:8

9何飞刚.BaTiO_3超细粉体的制备研究进展[J].应用化工,2010,39(11):1754-1757. 被引量:1

10何飞刚.介电温度稳定型BaTiO_3基陶瓷材料的研究进展[J].应用化工,2010,39(12):1918-1921.

1陈翀.高碳铬铁矿热炉煤气净化系统设计[J].冶金能源,2013,32(6):53-55. 被引量:2

2杜文轩,袁军年,李发荣,邬建国.石灰窑上料系统的改造[J].纯碱工业,2006(1):41-42.

3姚福国.关于喷粉罐主要工艺参数的确定[J].鞍钢技术,1997(6):14-17. 被引量:1

4王亚利.宣钢1~#、2~#链箅机-回转窑设备改造[J].烧结球团,2012,37(4):41-44. 被引量:1

5黄文莉,邝国春,杨惠.金属铽制备过程中影响金属铽收率因素探讨[J].江西有色金属,2004,18(1):28-30.

6一种电解生产铝锆合金的方法[J].世界有色金属,2005(2):67-67.

7罗岚,罗会秋,周浪.提高炉外铝热法制取铌铁收率的研究[J].材料导报,2005,19(F05):407-409. 被引量:1

8张爱明,焦刚.长钢高炉炉役后期的生产实践[J].炼铁技术通讯,2006,0(2):14-15.

9任益民,蒋光勤,胡渊明,刘建平.净化过程锌水解的控制及处理[J].有色冶炼,2001,30(5):108-110. 被引量:1

10田君,尹敬群.重稀土矿浸出液草酸沉淀的研究[J].湿法冶金,1996,15(2):16-19. 被引量:11

Basic Information:

DOI:

Chinese Library Classification Number:TF845.044[冶金工程—有色金属冶金]

Citation Information:

The paper briefly describes the bench scale test and 3 000 A electrolyzer pro duction of Pr metal by electrolysis of Pr oxide. The influence of electrolyte composition,electrolysis temperature, cathode current density and feedrate on the production efficiency is discussed. The practice shows that the electrolyzer has worked continuously and stably on a self-heating basis.The daily output of Pr metal per electrolyzer reached 65~70kg,metal re covery 90%,current efficiency>80%.

quote

GB/T 7714-2015 [1] OU Yang-yu-ping, WANG Yi-jun, RUAN Jian-hong, et al. Preparation of Pr Metal by Electrolysis of Pr Oxide Research and Industrial Practice[J]. Rare Metals and Cemented Carbides, 1997(3): 18-20.
MLA [1] OU Yang-yu-ping, et al., "Preparation of Pr Metal by Electrolysis of Pr Oxide Research and Industrial Practice." Rare Metals and Cemented Carbides, no. 3, 1997, pp. 18-20.
APA [1] OU Yang-yu-ping, WANG Yi-jun, RUAN Jian-hong, & SHU Bin. (1997). Preparation of Pr Metal by Electrolysis of Pr Oxide Research and Industrial Practice. Rare Metals and Cemented Carbides(3), 18-20.
IEEE [1] OU Yang-yu-ping, WANG Yi-jun, RUAN Jian-hong, and SHU Bin, "Preparation of Pr Metal by Electrolysis of Pr Oxide Research and Industrial Practice," Rare Metals and Cemented Carbides, no. 3, pp. 18-20, 1997. keywords: {electrolysis of Pr_6O, Pr metal, technology, industrial practice}