Study on La-reduction and Ce-reduction of the Enriched Oxides of Thulium Ytterbium and Lutecium AITranslate
Abstract AITranslate
The basic thermodynamic conditions of the process on producing ytterbium metal from the enriched oxides of Thulium,Ytterbium and Lutecium by La-reduction and Ce reduction have been calculated and reduction experiments were successfully carried out. The experiment results showed that under proper technical conditions, the ytterbium metal of more than 98% purity could be obtained in laboratory with direct recovery of 85%~90%.In this paper, behaviour of main rare earths components and other impurities during the reduc tion and their distribution in products have been investigated. Application comparison between La-reduction and Ce-reduction was breifly made.
KeyWords AITranslate
1张玻,贾江涛,廖春生,严纯华.电极液酸度及稀土浓度对硫酸体系电解还原提纯镱的影响[J].中国稀土学报,2006,24(1):116-119. 被引量:4
2郝占忠,许林成.选择性还原铥-镱-镥富集物制备金属镱和铥[J].中国有色金属学报,2018,28(12):2590-2597.
1廖春发,焦芸芬,邱定蕃,薛济来.Cyanex272-P_(507)浸渍树脂协同萃取色层分离铥镱镥的研究[J].中国稀土学报,2007,25(2):249-252. 被引量:11
2廖春发,梁勇,焦芸芬,薛济来.Cyanex272浸渍树脂萃取色层法分离铥、镱、镥[J].稀有金属,2007,31(6):824-828. 被引量:7
3焦芸芬,何小林,廖春发,姜平国.近十年来重稀土元素分离与提纯技术研究进展[J].稀土,2013,34(4):74-79. 被引量:13
4许晓芳,谭全银,刘丽丽,许开华,李金惠,王志石.稀土元素分离与提纯技术研究现状及展望[J].环境污染与防治,2019,41(7):844-851. 被引量:13
1吴炳乾,张耀文.镧热还原铥镜镥富集物时杂质行为的讨论[J].江西有色金属,1997,11(2):34-37. 被引量:1
2丁晓玲,吴炳乾.铈热还原铥镱镥富集物制取金属镱的热力学探讨[J].南方冶金学院学报,1996,17(3):204-209. 被引量:2
3杨凤丽,邓佐国,徐廷华.铥镱镥富集物萃取分离优化工艺与传统工艺分析比较[J].江西理工大学学报,2007,28(3):6-9. 被引量:4
4邓汝富,方诚厚,吴炳乾,肖房春,张文.用氧化镱富集物制取金属镱的工艺研究[J].稀有金属,1996,20(4):269-272. 被引量:5
5邓汝富,方诚厚,吴炳乾,肖房春,张文.用氧化镱富集物制取金属镱的热力学分析[J].稀有金属,1996,20(5):397-399. 被引量:2
6简讯[J].稀土信息,1997,3(6):7-7.
7刘大春,杨斌,戴永年,杜国山,唐万启,韩龙.从富铟渣提取金属铟的研究[J].稀有金属,2005,29(4):574-577. 被引量:25
8戴兴征,杨美彦,曾鹏,陈国木,黄孟阳,李国峰,王洪亮.高铁锌精矿焙砂强化浸出过程中铁的行为走向研究[J].矿冶工程,2012,32(2):96-99. 被引量:3
9李洪枚.用硫酸从废旧稀土荧光粉中浸出稀土[J].湿法冶金,2010,29(3):188-190. 被引量:15
10黄美松,成维,杨露辉,贾帅广.高纯金属镱的制备工艺研究[J].矿冶工程,2013,33(6):94-96. 被引量:7
Basic Information:
DOI:
Chinese Library Classification Number:TF845.031[冶金工程—有色金属冶金]
Citation Information:
The basic thermodynamic conditions of the process on producing ytterbium metal from the enriched oxides of Thulium,Ytterbium and Lutecium by La-reduction and Ce reduction have been calculated and reduction experiments were successfully carried out. The experiment results showed that under proper technical conditions, the ytterbium metal of more than 98% purity could be obtained in laboratory with direct recovery of 85%~90%.In this paper, behaviour of main rare earths components and other impurities during the reduc tion and their distribution in products have been investigated. Application comparison between La-reduction and Ce-reduction was breifly made.
quote
| GB/T 7714-2015 | [1] WU Bing-qian, ZHANG Yao-wen, DING Xiao-ling. Study on La-reduction and Ce-reduction of the Enriched Oxides of Thulium Ytterbium and Lutecium[J]. Rare Metals and Cemented Carbides, 1997(3): 13-17. |
| MLA | [1] WU Bing-qian, et al., "Study on La-reduction and Ce-reduction of the Enriched Oxides of Thulium Ytterbium and Lutecium." Rare Metals and Cemented Carbides, no. 3, 1997, pp. 13-17. |
| APA | [1] WU Bing-qian, ZHANG Yao-wen, & DING Xiao-ling. (1997). Study on La-reduction and Ce-reduction of the Enriched Oxides of Thulium Ytterbium and Lutecium. Rare Metals and Cemented Carbides(3), 13-17. |
| IEEE | [1] WU Bing-qian, ZHANG Yao-wen, and DING Xiao-ling, "Study on La-reduction and Ce-reduction of the Enriched Oxides of Thulium Ytterbium and Lutecium," Rare Metals and Cemented Carbides, no. 3, pp. 13-17, 1997. keywords: {La-reduction, Ce-reduction, enriched oxides of Thulium, Ytterbium and Lutecium, Ytterbium metal,thermodynamic condition} |