Preparation and Sintering of Doped Ceria Powder AITranslate

Northwest Nonferrous Metal Research Institute;Northwest Nonferrous Metal Research Institute;Northwest Nonferrous Metal Research Institute
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

This paper presents the results of preparation and sintering of yttria doped ceria powder,and describes the effects of main technical parameters on its properties.

KeyWords AITranslate

doped ceria powder yttria doping preparation sintering

1[1]RAMANARAYANEM T, et al. Proceedings of the 2nd International Symposium on Ionic and Mixed Conducting Ceramics[C]. San Francisco: The Electrochemical Soviety, Princeton 1994:448.

2[2]DOKIYA M, et al. Procedings of the 4th International Symposium on Solid Oxide Fuel Cells[C]. Yokohama Japan:The Electrochemical Society, 1995:1 028.

3[3]DOKIYA M, et al. Procedings of the 4th international Symposium on Solid Oxide Fuel Cells[C]. Yokohama Japan: The. Electrochemical Society, 1995:1 062.

4[4]MOGENSEN M, et al. Physical Properties of Mixed Conductor Solid Oxide Fuel Cell Anode of Doped CeO2 [J]. J Electrochem Soc, 1994,141:2 122.

5[5]CHEN C C, et at. Synthesis and Characterigation of YSZ Thin Film Electrolytes[J]. Solid state lonics, 1994,70-71:101.

6[6]BALAGS G B, et al. Impeaance Studies of Rare Earth Oxides Doped Ceria[J]. Solid State Ionics, 1995,76.

7[7]HERLE J V, et al. Fabrication and sintering of Fine yttria-Doped Ceria Powder[J]. J Am Ceram SOc 1997.80;933.

1宋晓岚,何希,杨海平,屈一新,曲鹏,邱冠周.掺杂纳米CeO_2基材料应用研究新进展[J].云南大学学报:自然科学版,2005,27(S1):33-37.

2张伟南,陈栋华.草酸盐在无机功能材料中的应用[J].中南民族大学学报:自然科学版,2004,23(2):29-32. 被引量:3

3崔成万,张德新,贾丹彬,戴文斌,于景坤.氧化铈/氧化钇复合材料的制备与性能[J].材料科学,2017,7(1):114-123.

1黄连荣,陈栋华,彭玉华.不同制备方法的CuC_2O_4-ZnC_2O_4·2H_2O的热行为和热分解动力学[J].中南民族大学学报:自然科学版,2004,23(3):12-16. 被引量:1

2闪海威,陈栋华,唐万军.MC_2O_4(M=Mn、Fe、Co、Ni、Cu、Zn)的热力学及其热分析动力学[J].物理化学学报,2005,21(9):1001-1005. 被引量:5

3刘春静,魏雨,郝顺利,王永明,王新.锰锌铁氧体纳米粉体的液相制备及磁性能[J].磁性材料及器件,2008,39(2):51-54.

1周喜,陈海焱,卢成渝,袁书林.流化床气流磨制备超细氧化铈粉末[J].粉末冶金技术,2011,29(1):46-49. 被引量:8

2刘志强,梁振锋,李杏英.碳铵沉淀法制备纳米氧化铈的研究[J].稀土,2006,27(5):11-14. 被引量:11

3朱达川,胡盛东,涂铭旌,庄稼,刘资甫.机械力固相化学反应法制备纳米氧化铈粉末[J].四川稀土,2004(1):6-9.

Basic Information:

DOI:

Chinese Library Classification Number:TF123.25[冶金工程—粉末冶金];TM911.4[电气工程—电力电子与电力传动]

Citation Information:

This paper presents the results of preparation and sintering of yttria doped ceria powder,and describes the effects of main technical parameters on its properties.

quote

GB/T 7714-2015 [1] HUANG Hong, LIU Jin-wei, HUANG Jin-chang. Preparation and Sintering of Doped Ceria Powder[J]. Rare Metals and Cemented Carbides, 2000(1): 31-34.
MLA [1] HUANG Hong, et al., "Preparation and Sintering of Doped Ceria Powder." Rare Metals and Cemented Carbides, no. 1, 2000, pp. 31-34.
APA [1] HUANG Hong, LIU Jin-wei, & HUANG Jin-chang. (2000). Preparation and Sintering of Doped Ceria Powder. Rare Metals and Cemented Carbides(1), 31-34.
IEEE [1] HUANG Hong, LIU Jin-wei, and HUANG Jin-chang, "Preparation and Sintering of Doped Ceria Powder," Rare Metals and Cemented Carbides, no. 1, pp. 31-34, 2000. keywords: {doped ceria powder;yttria doping;preparation;sintering}