Present Status of China's Tungsten Industry and Its Prospect AITranslate

Xiamen Tungsten Industry Co., Ltd.
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Preliminary analysis is made of the present status and prospect of China's tungsten industry To vitalize its development it is necessary to strengthen the management, deepen the reform,restructure the enterprises, change the operation way and rely on the scientific and technical progress.

KeyWords AITranslate

China tungsten industry present status prospect

1中国钨业协会.改革体制 拯救钨业[J].中国钨业,1998,(6):1-1.

2曾益敏,徐贵云,李显明,贾国治.我国钨矿山的现状与出路[J].中国钨业,1997,0(Z1):2-7. 被引量:2

3方略.中国钨工业集团化经营初探[J].中国钨业,1998(1):4-7. 被引量:1

4边万增,韩晓庆,彭如清,段普元.中国钨制品出口现状及展望[J].中国钨业,1997,0(3):3-6. 被引量:4

5陈勇志.我国硬质合金业存在的问题和对今后发展的思考[J].中国钨业,1997,0(11):3-8. 被引量:1

1孔昭庆.论中国钨业之科学发展[J].中国钨业,2004,19(3):1-4. 被引量:1

2杨召会.我国钨业发展存在的问题[J].中国金属通报,2008,0(10):11-11. 被引量:1

3文昱,冯金强.我国钨业发展现状与展望[J].科技广场,2014(4):224-227. 被引量:2

4许文渊,谢国勋.我国钨资源形势分析及钨业发展对策与建议[J].中国钨业,1999,14(5):56-59. 被引量:3

5祖芸.构筑发展平台 重塑世界钨都 中国·赣州钨业发展战略研讨会召开[J].中国钨业,2004,19(6):44-44.

6孔昭庆.钨价回归与资源危机[J].中国钨业,2005,20(3):1-5. 被引量:7

7周菊秋.“十五”期间我国钨工业发展概述及“十一五”期间我国钨工业发展规划初探[J].中国钨业,2006,21(5):1-5. 被引量:3

8孔昭庆.我国钨业发展的新阶段与可持续发展的科学建议[J].中国钨业,2005,20(1):4-8. 被引量:4

9我国钨产量预计突破8万t[J].国外金属矿选矿,2005,42(2):44-44.

10左铁镛.树立科学发展观 实现我国钨业可持续发展[J].中国钨业,2008,23(1):6-9. 被引量:11

Basic Information:

DOI:

Chinese Library Classification Number:F426.32[经济管理—产业经济]

Citation Information:

Preliminary analysis is made of the present status and prospect of China's tungsten industry To vitalize its development it is necessary to strengthen the management, deepen the reform,restructure the enterprises, change the operation way and rely on the scientific and technical progress.

quote

GB/T 7714-2015 [1] HUANG Cheng-tong. Present Status of China's Tungsten Industry and Its Prospect[J]. Rare Metals and Cemented Carbides, 2000(1): 35-38.
MLA [1] HUANG Cheng-tong. "Present Status of China's Tungsten Industry and Its Prospect." Rare Metals and Cemented Carbides, no. 1, 2000, pp. 35-38.
APA [1] HUANG Cheng-tong. (2000). Present Status of China's Tungsten Industry and Its Prospect. Rare Metals and Cemented Carbides(1), 35-38.
IEEE [1] HUANG Cheng-tong, "Present Status of China's Tungsten Industry and Its Prospect," Rare Metals and Cemented Carbides, no. 1, pp. 35-38, 2000. keywords: {China;tungsten industry;present status;prospect}