daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Fully Integrated Photodetector Array Based on an Electrochemically Exfoliated, Atomically Thin MoS2 Film for Photoimaging AITranslate

Huazhong University of Science and Technology; Huazhong University of Science and Technology; Huazhong University of Science and Technology; Huazhong University of Science and Technology; Huazhong University of Science and Technology; Huazhong University of Science and Technology; Huazhong University of Science and Technology; Huazhong University of Science and Technology; Huazhong University of Science and Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Despite the widespread interest in MoS2-based photodetectors over the past few years, use of a high-performance photoimaging device remains a major challenge due to the low yield and poor quality of the MoS2 film. In this paper, we demonstrate a simple method to fabricate a high-performance fully integrated photodetector array based on a large-area atomically thin MoS2 film for photoimaging. Here, the film is constructed by spin-coating of the MoS2 nanosheets, which are acquired via electrochemical intercalation and sonication-assisted exfoliation. By precisely controlling this process, semiconducting few-layered MoS2 nanosheets with pure phase can be obtained. High-performance photodetectors have been achieved for the TFSI-treated MoS2 film, as the responsivity reaches 1080 A/W, and the response/recovery time improved to 56/62 ms with high stability during the repeated on/off test. The overall performance is much better than that of previously reported photodetectors based on liquid-exfoliated MoS2 nanosheets. Furthermore, a fully integrated photoimaging device with a crossing structure and an effective pixel density of 460/cm2 has been fabricated based on the MoS2 film, and shows great potential for shape imaging with cross-talk suppression. We believe this work provides an approach to exploit the photodetector and image sensor based on layered materials.

KeyWords AITranslate

photodetector image sensor MoS2 film electrochemical exfoliation highresolution photoimaging twodimensional materials
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.1c01190

Chinese Library Classification Number:

Citation Information:

Despite the widespread interest in MoS2-based photodetectors over the past few years, use of a high-performance photoimaging device remains a major challenge due to the low yield and poor quality of the MoS2 film. In this paper, we demonstrate a simple method to fabricate a high-performance fully integrated photodetector array based on a large-area atomically thin MoS2 film for photoimaging. Here, the film is constructed by spin-coating of the MoS2 nanosheets, which are acquired via electrochemical intercalation and sonication-assisted exfoliation. By precisely controlling this process, semiconducting few-layered MoS2 nanosheets with pure phase can be obtained. High-performance photodetectors have been achieved for the TFSI-treated MoS2 film, as the responsivity reaches 1080 A/W, and the response/recovery time improved to 56/62 ms with high stability during the repeated on/off test. The overall performance is much better than that of previously reported photodetectors based on liquid-exfoliated MoS2 nanosheets. Furthermore, a fully integrated photoimaging device with a crossing structure and an effective pixel density of 460/cm2 has been fabricated based on the MoS2 film, and shows great potential for shape imaging with cross-talk suppression. We believe this work provides an approach to exploit the photodetector and image sensor based on layered materials.

quote

GB/T 7714-2015 [1] Bo Sun, Lingxian Kong, Guangliang Li, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.1c01190.
MLA [1] Bo Sun, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.1c01190.
APA [1] Bo Sun, Lingxian Kong, Guangliang Li, Qi Su, Xuning Zhang, Zhiyong Liu, Yang Peng, Guanglan Liao, & Tielin Shi. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.1c01190
IEEE [1] Bo Sun, Lingxian Kong, Guangliang Li, Qi Su, Xuning Zhang, Zhiyong Liu, Yang Peng, Guanglan Liao, and Tielin Shi, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.1c01190. keywords: {photodetector image sensor MoS2 film electrochemical exfoliation highresolution photoimaging twodimensional materials}