Diketopyrrolopyrrole-Based Chlorinated Bithiophene Polymers for Organic Solar Cells: Effect of Thiophene or Pyridine Flank Diketopyrrolopyrrole-Based Chlorinated Bithiophene Polymers for Organic Solar Cells: Effect of Thiophene or Pyridine Flank AITranslate

Osaka University; Osaka University; Osaka University; Osaka University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Although diketopyrrolopyrrole (DPP) conjugated polymers have been successfully explored in fullerene organic photovoltaics (OPVs) with high power conversion efficiency (PCE), their nonfullerene acceptor organic photovoltaics (NFOPVs) remain less investigated. Herein, we developed DPP-based polymers containing monochlorinated bithiophene (DPP2ThCl and DPP2PyCl), where the DPP unit was flanked by either thiophene or pyridine, respectively. DPP2ThCl showed a more extended photoabsorption and lower exciton binding energy in comparison to DPP2PyCl. The OPVs of these polymers blended with ITIC, IT-4F, Y6, and PC71BM revealed a PCE of 5.15% for DPP2ThCl:Y6, whereas the other blend gave lower values (0.07–4.07%). The superiority of DPP2ThCl:Y6 was rationalized by its enhanced planarity and crystallinity, smooth layer morphology, a low Flory–Huggins interaction parameter, and improved charge transport characteristics. We further analyzed the PCEs of all the blends by using machine learning, which identified the offset of highest occupied molecular orbital energies of donors and acceptors as the most important property. These findings highlight the importance of the structural manipulation of DPP-based polymers to improve the PCE of NFOPVs.

KeyWords AITranslate

diketopyrrolopyrrole chlorinated thiophene nonfullerene acceptor organic photovoltaics machine learning
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.2c00239

Chinese Library Classification Number:

Citation Information:

Although diketopyrrolopyrrole (DPP) conjugated polymers have been successfully explored in fullerene organic photovoltaics (OPVs) with high power conversion efficiency (PCE), their nonfullerene acceptor organic photovoltaics (NFOPVs) remain less investigated. Herein, we developed DPP-based polymers containing monochlorinated bithiophene (DPP2ThCl and DPP2PyCl), where the DPP unit was flanked by either thiophene or pyridine, respectively. DPP2ThCl showed a more extended photoabsorption and lower exciton binding energy in comparison to DPP2PyCl. The OPVs of these polymers blended with ITIC, IT-4F, Y6, and PC71BM revealed a PCE of 5.15% for DPP2ThCl:Y6, whereas the other blend gave lower values (0.07–4.07%). The superiority of DPP2ThCl:Y6 was rationalized by its enhanced planarity and crystallinity, smooth layer morphology, a low Flory–Huggins interaction parameter, and improved charge transport characteristics. We further analyzed the PCEs of all the blends by using machine learning, which identified the offset of highest occupied molecular orbital energies of donors and acceptors as the most important property. These findings highlight the importance of the structural manipulation of DPP-based polymers to improve the PCE of NFOPVs.

quote

GB/T 7714-2015 [1] Kakaraparthi Kranthiraja, Kazuharu Murotani, Fumiya Hamada, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c00239.
MLA [1] Kakaraparthi Kranthiraja, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c00239.
APA [1] Kakaraparthi Kranthiraja, Kazuharu Murotani, Fumiya Hamada, & Akinori Saeki. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c00239
IEEE [1] Kakaraparthi Kranthiraja, Kazuharu Murotani, Fumiya Hamada, and Akinori Saeki, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.2c00239. keywords: {diketopyrrolopyrrole chlorinated thiophene nonfullerene acceptor organic photovoltaics machine learning}