Derived Conduction Band Offset by Photoelectron Yield Spectroscopy and Its Quantitative Number for Efficiency Enhancement of Flexible, Cd-Free, and All-Dry Process Zn1–xMgxO:Al/Zn1–xMgxO/Cu(In,Ga)(S,Se)2 Solar Cells Derived Conduction Band Offset by Photoelectron Yield Spectroscopy and Its Quantitative Number for Efficiency Enhancement of Flexible, Cd-Free, and All-Dry Process Zn1–xMgxO:Al/Zn1–xMgxO/Cu(In,Ga)(S,Se)2 Solar Cells AITranslate
Abstract AITranslate
The actual conduction band offset (CBO) values of flexible, Cd-free, and all-dry process sputtered Zn0.88Mg0.12O:Al/sputtered Zn1–xMgxO buffer/Cu(In,Ga)(S,Se)2 solar cells on stainless steel were estimated using photoelectron yield spectroscopy. It is disclosed that the change of Mg content of the buffer from 0 to 0.41 yields the variation of its band gap (Eg) from 3.29 to 4.14 eV, thereby adjusting the CBO at the CIGSSe/Zn1–xMgxO interface from −0.20 to +0.60 eV. It is theoretically predicted that the derived CBO values are quantitatively optimized in a region from approximately −0.18 to +0.23 eV for high cell performance. The optimized and quantitative CBO values were then applied into the real devices. Consequently, high experimental conversion efficiencies up to about 15.0% (the highest one of 16.6%) are realized under the derived CBO values in a range from about +0.11 to +0.23 eV (or Mg content of Zn1–xMgxO buffer from 0.16 to 0.23), corresponding to the improved carrier lifetime and reduction of carrier recombination. On the other hand, the decreased CBO to −0.2 eV (using ZnO buffer) or lower and the increased CBO over +0.23 eV (Zn1–xMgxO buffer with an Mg content of over 0.23) generate large cliff-like and spike-like pn junctions, respectively, thereby increasing carrier recombination and reducing cell performances. Ultimately, the optimized derived CBO range was experimentally disclosed for the efficiency enhancement, which was numerically confirmed.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.2c00227
Chinese Library Classification Number:
Citation Information:
The actual conduction band offset (CBO) values of flexible, Cd-free, and all-dry process sputtered Zn0.88Mg0.12O:Al/sputtered Zn1–xMgxO buffer/Cu(In,Ga)(S,Se)2 solar cells on stainless steel were estimated using photoelectron yield spectroscopy. It is disclosed that the change of Mg content of the buffer from 0 to 0.41 yields the variation of its band gap (Eg) from 3.29 to 4.14 eV, thereby adjusting the CBO at the CIGSSe/Zn1–xMgxO interface from −0.20 to +0.60 eV. It is theoretically predicted that the derived CBO values are quantitatively optimized in a region from approximately −0.18 to +0.23 eV for high cell performance. The optimized and quantitative CBO values were then applied into the real devices. Consequently, high experimental conversion efficiencies up to about 15.0% (the highest one of 16.6%) are realized under the derived CBO values in a range from about +0.11 to +0.23 eV (or Mg content of Zn1–xMgxO buffer from 0.16 to 0.23), corresponding to the improved carrier lifetime and reduction of carrier recombination. On the other hand, the decreased CBO to −0.2 eV (using ZnO buffer) or lower and the increased CBO over +0.23 eV (Zn1–xMgxO buffer with an Mg content of over 0.23) generate large cliff-like and spike-like pn junctions, respectively, thereby increasing carrier recombination and reducing cell performances. Ultimately, the optimized derived CBO range was experimentally disclosed for the efficiency enhancement, which was numerically confirmed.
quote
| GB/T 7714-2015 | [1] Jakapan Chantana, Yu Kawano, Takahito Nishimura, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c00227. |
| MLA | [1] Jakapan Chantana, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c00227. |
| APA | [1] Jakapan Chantana, Yu Kawano, Takahito Nishimura, Abdurashid Mavlonov, Takayuki Negami, & Takashi Minemoto. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c00227 |
| IEEE | [1] Jakapan Chantana, Yu Kawano, Takahito Nishimura, Abdurashid Mavlonov, Takayuki Negami, and Takashi Minemoto, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.2c00227. keywords: {flexible and Cdfree Cu(In;Ga)(S;Se)2 thinfilm solar cell alldry process Zn1−xMgxO buffer Zn1−xMgxO:Al TCOShow More} |