Effects of Finishing Annealing Temperature on Deformation Texture and Mechanical Properties of Zr-4 Zirconium Alloy Tube AITranslate

School of Metallurgy and Engineering,Xi'an University of Architecure and Technology;State Nuclear BaoTi Zirconium Industry Company;National Center for Energy Research and Development of Nuclear Grade Zirconium;Shaanxi Key Laboratory of Nuclear Grade Zirconium
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The effects of annealing temperature on metallographic microstructure,deformation texture,contractile strain ratio(CSR)and Kearns coefficient Frof the finished Zr-4 zirconium alloy were studied.When the finished tube is annealed for stress relief at 450~500 ℃,the tube is in the recovery stage,and this process can not weaken deformation texture formed by crystal surface sliding due to metal deformation.Compared with the rolled tube,CSR value of the annealed tube at 450~500 ℃ has no significant change,and its Frvalue slightly increases with the increase of annealing temperature.At the annealing temperature of 500~530℃,the zirconium alloy tube is in the transition zone between the recovery stage and the recrystallization stage,and most of deformation texture is transformed into annealed texture,resulting in a sharp increase of Frvalue and CSR value.At the annealing temperature of 530~560 ℃,the zirconium alloy tube is in the stage of recrystallization,its microstructure is of equiaxed recrystallized morphology,and the original deformation texture has basically been completely replaced by annealed texture.However,the tube in the stage has not reached complete recrystallization,resulting in a slight increase of Frvalue and CSR value.

KeyWords AITranslate

Zr alloy tube Zr-4 finishing annealing temperature contractile strain ratio (CSR) Kearns coefficient Fr radial texture

1潘钱付,蒋明忠,戴训,王贯春,黄照华,赵文金.退火方式对N36锆合金包壳管性能的影响[J].金属热处理,2015,40(12):135-138. 被引量:3

2杨磊,惠松骁,叶文君,黄亮.TA18钛合金管材织构的测试与EBSD分析[J].稀有金属,2011,35(6):928-933. 被引量:14

3张旺峰,王玉会,李艳,曹春晓.高强度TA18合金管材性能评价与控制方法研究[J].稀有金属材料与工程,2012,41(7):1239-1242. 被引量:14

4彭继华,李文芳,Jean-Luc Bechade,R.Maury.织构对先进锆合金蠕变性能各向异性的影响[J].稀有金属,2008,32(1):1-6. 被引量:16

5彭继华,李文芳,Jean-Luc Bechade,Rauchy Morry.织构对锆合金拉伸和爆破性能的影响[J].材料研究与应用,2007,1(2):122-126. 被引量:10

1何伟,郭征,杜小平,马红征,杨军红.一种纯锆显微组织的新型显示方法[J].金属世界,2019(3):65-67.

2朱广伟,赵乙丞,赵帆,齐鹏,张志豪.张力退火对Zr–4合金织构和再结晶行为的影响[J].工程科学学报,2020,42(9):1174-1181. 被引量:2

3房永强,余泽利,白新房,张兵,张艺新,王柯.TA18钛合金管收缩应变比的测量不确定度评定[J].塑性工程学报,2021,28(12):230-236. 被引量:2

1赵帆,赵乙丞,齐鹏,张志豪.锆合金热挤压用防护润滑剂的试制与性能[J].工程科学学报,2021,43(2):232-238. 被引量:1

2田煜,许慧静,李进.金属材料力学性能测试中存在的不确定度分析[J].造纸装备及材料,2022,51(1):91-93. 被引量:1

3雷从一,毛建中,周惦武,张小民,王练.退火工艺对锆合金成形性能的影响[J].中国有色金属学报:英文版,2022,32(9):2908-2921.

4韩晓兰,刘战锋.大孔径钛合金管深孔套料钻削技术及应用[J].重型机械,2022(6):48-52.

1佟昕昕,王强,袁改焕,储林华,张天广,麻凯.径向压扁变形对Zr-4合金管材氢化物取向的影响[J].钛工业进展,2018,35(4):44-47.

2林辉.着眼长远 引领中国锆合金本地化生产[J].军工文化,2018,0(4):59-61.

3魏安妮,白朴存,佟乃强,刘飞,崔晓明.退火时间对3003铝合金织构及制耳的影响[J].内蒙古工业大学学报:自然科学版,2017,36(5):347-352. 被引量:1

4李剑飞,贾国朋,李细锋,梅琼风.蒙皮拉形中橘皮缺陷的研究进展[J].模具技术,2018(2):55-63. 被引量:4

5王承阳,董帝,滕宇阔,康聚磊,林婷.退火工艺对MHC钼合金板材组织和力学性能的影响[J].金属热处理,2018,43(7):180-183. 被引量:7

6丁岚,张乔,于军辉.浅析锆合金管材轧制的生产效率控制[J].科技视界,2018(19):236-237.

7李亚萍,肖柱,雷前,周哲远,李周.高强高导Cu-Mg-Ca合金加工过程中组织结构演变[J].中国有色金属学报,2018,28(3):547-555. 被引量:4

8宝钢特钢成功交付超长薄壁镍基合金管材[J].特种铸造及有色合金,2018,0(4):401-401.

9苏娟华,邵鹏,任凤章.TA10钛合金高温流变行为及拉伸性能[J].材料热处理学报,2018,39(6):14-20. 被引量:6

10陈高红,李国爱,陈军洲,汝继刚,何维维.轧制组织特征对7B50-T7751铝合金厚板断裂韧性的影响[J].轻合金加工技术,2018,46(6):29-33. 被引量:5

Basic Information:

DOI:

Chinese Library Classification Number:TG146.414[金属学及工艺—金属材料]

Citation Information:

The effects of annealing temperature on metallographic microstructure,deformation texture,contractile strain ratio(CSR)and Kearns coefficient Frof the finished Zr-4 zirconium alloy were studied.When the finished tube is annealed for stress relief at 450~500 ℃,the tube is in the recovery stage,and this process can not weaken deformation texture formed by crystal surface sliding due to metal deformation.Compared with the rolled tube,CSR value of the annealed tube at 450~500 ℃ has no significant change,and its Frvalue slightly increases with the increase of annealing temperature.At the annealing temperature of 500~530℃,the zirconium alloy tube is in the transition zone between the recovery stage and the recrystallization stage,and most of deformation texture is transformed into annealed texture,resulting in a sharp increase of Frvalue and CSR value.At the annealing temperature of 530~560 ℃,the zirconium alloy tube is in the stage of recrystallization,its microstructure is of equiaxed recrystallized morphology,and the original deformation texture has basically been completely replaced by annealed texture.However,the tube in the stage has not reached complete recrystallization,resulting in a slight increase of Frvalue and CSR value.

quote

GB/T 7714-2015 [1] LI Xiao-ning, WANG Kuai-she, YU Jun-hui, et al. Effects of Finishing Annealing Temperature on Deformation Texture and Mechanical Properties of Zr-4 Zirconium Alloy Tube[J]. Rare Metals and Cemented Carbides, 2018(4): 73-77.
MLA [1] LI Xiao-ning, et al., "Effects of Finishing Annealing Temperature on Deformation Texture and Mechanical Properties of Zr-4 Zirconium Alloy Tube." Rare Metals and Cemented Carbides, no. 4, 2018, pp. 73-77.
APA [1] LI Xiao-ning, WANG Kuai-she, YU Jun-hui, & WANG Chen-yang. (2018). Effects of Finishing Annealing Temperature on Deformation Texture and Mechanical Properties of Zr-4 Zirconium Alloy Tube. Rare Metals and Cemented Carbides(4), 73-77.
IEEE [1] LI Xiao-ning, WANG Kuai-she, YU Jun-hui, and WANG Chen-yang, "Effects of Finishing Annealing Temperature on Deformation Texture and Mechanical Properties of Zr-4 Zirconium Alloy Tube," Rare Metals and Cemented Carbides, no. 4, pp. 73-77, 2018. keywords: {Zr alloy tube;Zr-4;finishing annealing temperature;contractile strain ratio (CSR);Kearns coefficient;Fr;radial texture}